Sub-microfibers and nanofibers produce more breathable fabrics than coarse fibers and are therefore widely used in the textiles industry. They are prepared by electrospinning using a polymer solution or melt. Solution electrospinning produces finer fibers but requires toxic solvents. Melt electrospinning is more environmentally friendly, but is also technically challenging due to the low electrical conductivity and high viscosity of the polymer melt. Here we describe the use of colorants as additives to improve the electrical conductivity of polylactic acid (PLA). The addition of colorants increased the viscosity of the melt by >100%, but reduced the electrical resistance by >80% compared to pure PLA (5 GΩ). The lowest electrical resistance of 50 MΩ was achieved using a composite containing 3% (w/w) indigo. However, the thinnest fibers (52.5 µm, 53% thinner than pure PLA fibers) were obtained by adding 1% (w/w) alizarin. Scanning electron microscopy revealed that fibers containing indigo featured polymer aggregates that inhibited electrical conductivity, and thus increased the fiber diameter. With further improvements to avoid aggregation, the proposed melt electrospinning process could complement or even replace industrial solution electrospinning and dyeing.
Electrospinning is widely used for the manufacture of fibers in the low-micrometer to nanometer range, allowing the fabrication of flexible materials with a high surface area. A distinction is made between solution and melt electrospinning. The former produces thinner fibers but requires hazardous solvents; whereas the latter is more environmentally sustainable because solvents are not required. However, the viscous melt requires high process temperatures and its low conductivity leads to thicker fibers. Here, we describe the first use of the biobased dyes alizarin; hematoxylin and quercetin as conductive additives to reduce the diameter of polylactic acid (PLA) fibers produced by melt electrospinning; combined with a biobased plasticizer to reduce the melt viscosity. The formation of a Taylor cone followed by continuous fiber deposition was observed for all PLA compounds; reducing the fiber diameter by up to 77% compared to pure PLA. The smallest average fiber diameter of 16.04 µm was achieved by adding 2% (w/w) hematoxylin. Comparative analysis revealed that the melt-electrospun fibers had a low degree of crystallinity compared to drawn filament controls—resembling partially oriented filaments. Our results form the basis of an economical and environmentally friendly process that could ultimately, provide an alternative to industrial solution electrospinning
The COVID-19 pandemic led to a huge demand for disposable facemasks. Billions were manufactured from nonbiodegradable petroleum-derived polymers, and many were discarded in the environment where they contributed to plastic pollution. There is an urgent need for biobased and biodegradable facemasks to avoid environmental harm during future disease outbreaks. Melt electrospinning is a promising alternative technique for the manufacturing of filter layers using sub-microfibers prepared from biobased raw materials such as polybutylene succinate (PBS). However, it is not yet possible to produce sub-micrometer PBS fibers or uniform nonwoven-like samples at the pilot scale, which hinders their investigation as filter layers. Further optimization of pilot-scale PBS melt electrospinning is therefore required. Here, we tested the effect of different parameters such as electric field strength, nozzle-to-collector distance and throughput on the final fiber diameter and sample uniformity during PBS melt electrospinning on a pilot-scale device. We also studied the effect of a climate chamber and an additional infrared heater on the solidification of PBS fibers and their final diameter and uniformity. In addition, a post-processing step, including a hot air stream of 90 °C for 30 s has been studied and successfully lead to a nonwoven-like structure including filaments that weld together without changing their structure. The finest fibers (1.7 µm in diameter) were produced at an applied electric field strength of −40 kV, a nozzle-to-collector distance of 5.5 cm, and a spin pump speed of 2 rpm. Three uniform nonwoven-like samples were tested as filter layers in a medical face mask by measuring their ability to prevent the transfer of bacteria, but the pore size was too large for effective retention. Our results provide insight into the process parameters influencing the suitability of melt-electrospun nonwoven-like samples as biobased and biodegradable filter materials and offer guidance for further process optimization.
The color of textile fibers is typically imparted by submersion in a high-temperature dye bath. However, the treatment of the effluent is challenging and the textile industry is therefore a major source of water pollution. Current fashion trends favor biobased polymers such as polylactic acid (PLA) but exhaust dyeing at high temperatures causes hydrolytic degradation, reducing the crystallinity and tenacity of the yarn. To preserve the mechanical properties of PLA-based textiles, an alternative to exhaust dyeing called dope dyeing can be used, wherein colorants are incorporated into the polymer matrix during melt spinning. We evaluated this process by dope dyeing PLA with several colorants, then testing the thermal, physical, and mechanical properties of the yarn and the physical properties of circular-knitted fabrics. Although the colorants affected the crystallization behavior at lower cooling rates, during the melt-spinning process, the drawing speed had a greater effect on the crystallinity and mechanical properties of the dyed yarn. Scanning electron microscopy revealed that the colorants were well dispersed in the PLA matrix. We found that the colorants did not affect the physical properties of the knitted fabric. Our results can be used to develop more environmentally beneficial dope-dyed PLA yarn with improved mechanical properties.
Melt electrospinning is a polymer processing technology for the manufacture of microfibers and nanofibers. Additives are required to reduce the melt viscosity and increase its conductivity in order to minimize the fiber diameter, and can also impart additional beneficial properties. We investigated the preparation of polybutylene succinate (PBS) microfibers incorporating different weight percentages of two multifunctional additives (the organic dye curcumin and inorganic silver nanoparticles) using a single-nozzle laboratory-scale device. We determined the influence of these additives on the polymer melt viscosity, electrical conductivity, degradation profile, thermal behavior, fiber diameter, and antibacterial activity. The formation of a Taylor cone followed by continuous fiber deposition was observed for compounds containing up to 3% (w/w) silver nanoparticles and up to 10% (w/w) curcumin, the latter achieving the minimum average fiber diameter of 12.57 µm. Both additives reduced the viscosity and increased the electrical conductivity of the PBS melt, and also retained their specific antibacterial properties when compounded and spun into fibers. This is the first report describing the effect of curcumin and silver nanoparticles on the properties of PBS fibers manufactured using a single-nozzle melt-electrospinning device. Our results provide the basis to develop environmentally benign antibacterial melt-electrospun PBS fibers for biomedical applications.
The demand is rising for colorants that are obtained from natural resources, tolerant to industrial processing methods, and meet color quality demands. Herein, we report how relevant properties such as thermal stability and photostability of the natural colorant alizarin can be improved by grafting it onto ZnO nanoparticles (NPs), allowing application in a warm extrusion process for the fabrication of polyamide fibers. For this study, ZnO NPs (diameter 2.0 ± 0.6 nm) were synthesized and subsequently functionalized with alizarin. The alizarin-coated ZnO NPs (i.e., dyed nanoparticles, DNPs) were characterized. Thermogravimetric analysis and ultraviolet–visible (UV–vis) studies revealed that alizarin coating accounts for ∼65% (w/w) of the total mass of the DNPs. A subsequent detailed characterization with Fourier transform infrared (FT-IR), 1H nuclear magnetic resonance (NMR), 13C cross-polarization magic angle spinning (CP-MAS) NMR, X-ray photoelectron spectroscopy (XPS), and quantum chemistry studies using various density functional theory (DFT) functionals and basis sets indicated that binding onto the ZnO NPs occurred predominantly via the catechol moiety of alizarin. Importantly, this grafting increased the thermal stability of alizarin with >100 °C, which allowed the processing of the DNPs into polyamide fibers by warm extrusion at 260 °C. Evaluation of the lightfastness of the DNP-dyed nylon fibers revealed that the changes in color quantified via the distance metric ΔE* of alizarin when embedded in a hybrid material were 2.6-fold better compared to nylon fibers that were directly dyed with alizarin. This reveals that the process of immobilization of a natural dye onto ZnO nanoparticles indeed improves the dye properties significantly and opens the way for a wide range of further studies into surface-immobilized dyes.