The present study investigated the microstructure, mechanical and corrosion behaviour of Al6061 alloy reinforced with nano zirconium diboride (ZrB2) particles. The stir casting route is carried out to fabricate the Al6061 metal matrix nanocomposites (AMMNCs) by varying 0 to 2 Wt% of ZrB2 nanoparticles. X-ray Diffraction (XRD)was used to study the crystalline size and phase distribution of AMMNCs. Scanning electron microscope (SEM) analysis reveals the uniform dispersion of ZrB2 nano particulates in AMMNCs. Ultimate tensile strength and yield strength, hardness of the AMMNCs were increased by 33.58%, 27.54%, and 40.57%, respectively, with the addition of ZrB2 nano particulates, while the elongation decreased to 46.03%. with the increase in ZrB2 Wt%. The corrosion rate of AMMNCs (2 Wt% ZrB2) decreased by 86% compared to Al6061 alloy. Fracture analysis of the samples showed that the fracture behaviour of Al6061 matrix alloy changed from ductile intergranular fracture to cleavage. The results show that the developed nanocomposite enhances mechanical properties and corrosion resistance with an increase in Wt% of reinforcement.
Titanium and its alloys are extensively used in automobile, aerospace and biomedical applications. There are many problems associated with the fusion welding of titanium. Thus, friction welding is an alternative technique for joining titanium without defects. In this study, Ti-6Al-4V (Grade 5 -Titanium alloy) rods were welded using a rotary friction process. Before welding, pre-heat treatments were carried in α - β and β conditions followed by stress relieving on Grade 5 -Titanium alloy rods and some rods were stress relieved after welding. After several trials, friction welding at rotational speed, 1500 rpm and 5 kN upset force obtained defect-free joints. α - β heat treatment enhanced ductility as compared with β heat treatment. α - β heat treatment lead formation of bimodal microstructure in the base metal and β heat treatment produced lamellar Coarse β grains with colonies of α within β grains. Among different heat treatment conditions, high hardness was observed in the α - β heat treatment condition with stress-relieving. Stress-relieving of the welds resulted in an improvement in the hardness because of β precipitates. Fracture morphology is brittle in β treated conditions and ductile in α - β conditions. All welded samples failed away from the weld region irrespective of heat treatments applied, this shows that the weld region is much stronger than the base region due to acicular α and β phases. Mechanical properties were correlated as evidenced by microstructural features.