In this work, the corrosion properties of 316L stainless steel (SS) obtained by selective laser melting (SLM) are analyzed. The electrochemical results of samples manufactured with an energy density between 40 and 140 J/mm3 are compared using different hatch distances and laser speeds. The analysis correlates the impact of the microstructure and processing defects of SLM 316L stainless steel on its behavior against corrosion. The optimal manufacturing conditions were selected considering the electrochemical results. Although the samples obtained with an energy density close to 90 J/mm3 show a high resistance to corrosion, their performance depends on the combination of selected parameters, obtaining the best results for an intermediate laser speed and a low hatch distance. These manufacturing conditions produce a higher breakdown potential, a faster repassivation of the steel and reduce the current density on electrochemical test.
3 May 2006 in Journal of Analytical Atomic Spectrometry
A flow-through UV reactor has been implemented in an automated flow-injection/stopped-flow manifold, and used for on-line generation of Se volatile derivatives prior to detection by quartz furnace atomic absorption spectrometry. The presence of a low molecular weight organic acid (formic or acetic) in the carrier was a necessary requirement so that efficient vapour generation was achieved. Stopped-flow conditions were employed with the aim of increasing the time for which the sample zone was subjected to UV irradiation while it was transported to the detector. The simultaneous formation of H2 during the photochemical decomposition of formic acid facilitated the atomization of the Se derivatives in the quartz furnace, and therefore the addition of H2 to the carrier gas, which is necessary for efficient atomisation, could be eliminated. Nevertheless, the presence of H2 in the carrier gas (Ar) was required for efficient atomisation when using acetic acid as carrier. This manifold allowed a sample throughput of 26 h−1 with a detection limit of 0.5 ng mL−1 Se and a repeatability, expressed as relative standard deviation, of 4%. Effect of concomitants in the online generation of Se vapours with the new manifold was investigated. Chloride salts of alkaline and alkaline-earth elements did not interfere at concentrations up to 10 000 mg L−1, but nitrate salts caused a positive effect. Tolerance of typical hydride-forming elements such as As and Sn was much higher with UV vapour generation as compared to chemical hydride generation. The presence of Cu(II) was critical since interference effects are observed from 0.05 mg L−1, but tolerance of Ni(II) was greater with UV vapour generation.