Magnetism plays a pivotal role in many biological systems. However, the intensity of the magnetic forces exerted between magnetic bodies is usually low, which demands the development of ultra-sensitivity tools for proper sensing. In this framework, magnetic force microscopy (MFM) offers excellent lateral resolution and the possibility of conducting single-molecule studies like other single-probe microscopy (SPM) techniques. This comprehensive review attempts to describe the paramount importance of magnetic forces for biological applications by highlighting MFM’s main advantages but also intrinsic limitations. While the working principles are described in depth, the article also focuses on novel micro- and nanofabrication procedures for MFM tips, which enhance the magnetic response signal of tested biomaterials compared to commercial nanoprobes. This work also depicts some relevant examples where MFM can quantitatively assess the magnetic performance of nanomaterials involved in biological systems, including magnetotactic bacteria, cryptochrome flavoproteins, and magnetic nanoparticles that can interact with animal tissues. Additionally, the most promising perspectives in this field are highlighted to make the reader aware of upcoming challenges when aiming toward quantum technologies.
27 January 2021 in ACS Applied Materials & Interfaces
Multiferroic heterostructures based on the strain-mediated mechanism present ultralow heat dissipation and large magnetoelectric coupling coefficient, two conditions that require endless improvement for the design of fast nonvolatile random access memories with reduced power consumption. This work shows that a structure consisting of a [Pb(Mg1/3Nb2/3)O3]0.7-[PbTiO3]0.3 (001) substrate on which a crystalline FeGa(001)/MgO(001) bilayer is deposited exhibits a giant magnetoelectric coupling coefficient of order 15 × 10–6 s m–1 at room temperature. That result is a 2-fold increment over the previous highest value. The spatial orientation of the magnetization vector in the epitaxial FeGa film is switched 90° with the application of electric field. The symmetry of the magnetic anisotropy is studied by the angular dependence of the remanent magnetization, demonstrating that poling the sample generates a switchable uniaxial magnetoelastic anisotropy in the film that overcomes the native low 4-fold magnetocrystalline anisotropy energy. Magnetic force microscopy shows that the switch of the easy axis activates the displacement of domain walls and the domain structures remain stable after that point. This result highlights the interest in single-crystalline structures including materials with large magnetoelastic coupling and small magnetocrystalline anisotropy for low-energy-consuming spintronic applications.
The patterning-induced changes in the magnetic anisotropy and hysteresis of epitaxial (100)-oriented Cu/Ni(9, 10, 15 nm)/Cu planar nanowires have been quantified. When the Ni films are patterned into lines, strain relaxation leads to a thickness-dependent net in-plane anisotropy transverse to the lines. The magnetoelastic anisotropy was found from the three-dimensional strain state measured directly by synchrotron x-ray diffraction and has a value of for 10-nm-thick nanowires. The angular dependence of the remanence of the nanowires indicates that the in-plane easy direction is the result of the competition between the cubic magnetocrystalline anisotropy and a uniaxial anisotropy that includes shape and magnetoelastic effects. The patterning-induced changes in magnetoelastic anisotropy, combined with the shape and magnetocrystalline anisotropies, quantitatively explain the net anisotropy of the nanowires. Thus by controlling the film thickness and wire orientation, the easy axis direction of the nanowires may be controlled.
The role of the strain state in epitaxial (001)-oriented Cu/Ni(14 nm)/Cu rings is investigated using a combination of magnetic force microscopy and finite-element calculations. Rings with an external diameter of 3 and 2 m and linewidth larger than 400 nm show two different structures: domains with magnetization oriented in the radial direction exist at the inner and outer radius, separated by an area in the interior of the ring consisting of stripe domains with perpendicular magnetization. The former is the sole magnetic structure observed for nm. Micromagnetic calculations on narrow-linewidth structures indicate that the radial domain-wall structure consists of elliptical Bloch lines with a shorter and longer length along the tangential and radial directions, respectively. Finite-element calculations show that the anisotropic relaxation of the in-plane strain is larger at the ring inner and outer edges than in the interior part of the ring and accounts for the reorientation of the magnetization direction.
The magnetoelastic (ME) stresses for a series of epitaxial films are reported. The direct measurement of the stresses in the (001) plane allows determination of the irreducible ME stress that accounts for the breaking of the in-plane square symmetry. has been determined as a function of the applied magnetic field and the temperature for ranging from 5 to . The temperature dependence of is proportional to the square power of the reduced magnetization and the value increases with the internal stress. These experimental observations are explained considering the tetragonal distortion of the nickel caused by the epitaxial strain that the copper lattice introduces in the nickel layers.