The diversity of aromatic building blocks, bridging groups, and their connection patterns determines the richness of macrocyclic host molecules (MHMs). The MHMs with new aromatic building blocks reported in the last ten years were summarized and discussed.
14 June 2019 in Beilstein Journal of Nanotechnology
Tb2.96−xCe0.04GdxAl5O12 phosphors were synthesized through solid-state reactions. The influence of Gd3+ on the luminescence was investigated. Under the excitation at 460 nm, Tb2.96Ce0.04Al5O12 shows the characteristic emission band of Ce3+ with a peak wavelength at about 554 nm. After co-doping Gd3+ into Tb2.96Ce0.04Al5O12, the peak wavelength of the Ce3+ emission band shifts to longer wavelengths, which is induced by the increasing crystal field splitting. However, the Ce3+ emission intensity also decreases because the substitution of Tb3+ with Gd3+ causes lattice deformation and generates numerous structural and chemical defects. By comparing the light parameters of white light-emitting diodes (WLEDs) containing Y2.96Ce0.04Al5O12, Tb2.96Ce0.04Al5O12 and Tb2.81Ce0.04Gd0.15Al5O12 phosphors, we can find that the WLED containing the Tb2.81Ce0.04Gd0.15Al5O12 phosphor generates warmer light than the WLEDs containing Y2.96Ce0.04Al5O12 and Tb2.96Ce0.04Al5O12 phosphors. Moreover, the WLEDs fabricated by integrating a blue LED chip and Ce3+/Gd3+-co-doped Tb3Al5O12 phosphors show outstanding colour stability when driven under different currents.
27 May 2019 in Journal of Materials Science: Materials in Electronics
We synthesized Dy 3+ doped SrLaGa 3 O 7 phosphors via a sintering process at 1350 °C under atmosphere. The X-ray diffraction data demonstrate that they have the pure tetragonal phase, meaning the successful substitution of Dy 3+ in SrLaGa 3 O 7 host. Monitoring at 572 nm, Dy 3+ doped SrLaGa 3 O 7 phosphors show a series of excitation bands within 275–475 nm. Exciting at 342 nm, Dy 3+ doped SrLaGa 3 O 7 phosphors show emission bands in the range of 450–700 nm. The emission bands respectively locate in blue, yellow and right light regions, which respectively correspond to 4 F 9/2 → 6 H 15/2 , 4 F 9/2 → 6 H 13/2 and 4 F 9/2 → 6 H 11/2 transitions of Dy 3+ . The concentration quenching is induced by dipole-dipole interactions among neighboring Dy 3+ ions. There is only one peak in the thermoluminescence glow curves of Dy 3+ doped SrLaGa 3 O 7 phosphors, indicating that there is only one type of trap center in these phosphors. The trap depth is calculated to be 0.754 eV.