With the rapid development of robotics, robots gradually replace people to complete various tasks. Grasping is one of the most common tasks in industry and daily life. In addition to typical pick-and-place task, grasping a tool is the basis for performing other tasks, such as grabbing the key to open the door, grabbing a hammer to nail, etc. The robotic grippers are the manipulator in which the robot completes the grasp. Their performance characteristics have a significant impact on work efficiency because they are the parts interacting with the grasping objects directly. Therefore, this paper researches on robotic gripper and its related technology from the following aspects. First of all, the current robotic gripper type is analyzed in detail. Second, the research status of the most promising robotic gripper is reviewed widely. Third, the critical technology of robotic gripper is studied deeply. Finally, the analysis of robotic gripper development trend is performed prospectively.
26 May 2022 in Nondestructive Testing and Evaluation
Thermal barrier coatings (TBCs) is a typical brittle, heterogeneous, multilayer structure material. The heat-loading effect during service will lead to premature peeling failure of the coating. The main failure modes are cracking and interface spalling failure of ceramic coating. The failure of the TBCs is mainly caused by the initiation, propagation and connection of microcracks. In this study, acoustic emission technique (AE) combined with microscopic morphology are used to study the failure process of TBCs under tensile load, and fast Fourier transform (FFT) and wavelet transform are used to identify the crack damage mode of TBCs. The results show that the tensile failure process of the TBCs is that the crack firstly sprouts on the surface of the ceramic coating and then spreads to the interface of the ceramic coating/bond coating. After reaching the interface, the crack will grow and propagate along with the interface, eventually leading to ceramic coating is peeled off; The failure process of the TBCs is divided into four steps. Meanwhile, the spectrum analysis shows that the frequency component of the substrate is around .020 MHz, the frequency component of the surface crack is .20–.25 MHz, and the interface crack is .15–.20 MHz.
7 April 2023 in Journal of Thermal Spray Technology