The mineral surface structure and ions’ interaction were of significant interest to understanding mineral dissolution and reaction. In this study, X-ray photoemission spectroscopy combined with ICP emission spectrometer was used to investigate the influence of the leaching reaction conditions of 8 M dilute sulfuric acid and 12 M concentrated sulfuric acid on the surface chemical composition, chemical (valence) state and ion distribution of Columbite-(Fe) (FeNb2O6). The binding energy of the cations (Fe, Nb) bonding with different anions (O2−, SO42−) and the ratio of Fe3+/Fe2+ oxidation–reduction provided direct understanding of Fe and Nb releasing from the mineral surface during leaching. The results showed that the binding energy of the Nb5+-O bond was much smaller than that of Nb5+-SO4, and the binding energy decreased in sequence as Nb5+-O < Fe2+-O < Fe3+-O and increased in sequence as Fe3+-SO4 < Fe2+-SO4 < Nb5+-SO4. The mineral surface reaction during the leaching could be expressed with the formula: Fe-O + H2SO4 → Fe-SO4 + H2O, Nb-O + H2SO4 → Nb-SO4 + H2O. The results also revealed that Nb dissolution from Columbite-(Fe) occurred more easily compared to Fe. Nb dissolution from the mineral was owed to the content of H+ in solution, and increasing the H+ concentration could promote the dissolution. For Fe dissolution from the mineral, the oxidation potential could play an effective role in enhancement dissolution.
17 April 2024 in Transactions of the Indian Institute of Metals
The acceleration of the carburizing and melting processes in reduced iron is critical for reducing energy consumption and CO2 emissions produced by the steel industry. The aims of the study were to clarify the carbon dissolution reactions and diffusion processes in molten slag. A combined approach utilizing Raman spectroscopy and XPS was employed to investigate the relationship between carbon-containing species and slag composition in the CaO-SiO2-Al2O3 slag system. The Raman spectra indicated that carbon dissolved in slag in the form of carbides, carbonates, and graphitic structures. The proportion of carbide ions in the slag increased from 64.2% to 74.7%, and the proportion of graphitic structures decreased from 19.7% to 7.4% as the slag's basicity increased. The carbon dissolution mechanism in slag involved the reaction of carbon with dissolved oxide ions and oxygen-containing anions in the slag. This formed carbon-containing species such as CO32-, C22-, and graphitic structures that diffused in the slag and subsequently underwent carburization and deposition at the iron interface.