Performance degradation is one of the crucial difficulties for the market of organic solar cell (OSC) devices. These deteriorative characteristics can be attributed to many factors, mainly to the chemical reactivity of the device multiple layers with the environment. Here, we investigate the performance of a standard OSC device made of the polymer poly(3-hexylthiophene-2,5-diyl) and the fullerene [6,6]-phenyl-C61-butyric-acid-methyl-ester (P3HT:PCBM) as a photoactive layer in a high humidity environment (53%) within 100 days divided into three periods. The results confirm that the OSC devices’ encapsulations should be completed immediately after the fabrication due to fast chemical degradation of the photoactive layer, which reduces the Jsc by 15% after 40 mins of fabrication. We also found that the FF has been reduced by 17.36% from its initial value after 1152 hours due to a deficiency of the interfacial charge transfer between the multiple layers of the device. Finally, the performance of the device’s decays to zero after 2400 hours.
This study examines the impact of incorporating a thin gold (Au) nanofilm as an interfacial buffer layer between the anode and the active layer in poly(3-hexylthiophene-2,5-diyl):[6,6]-phenyl-C61-butyric acid methyl ester (P3HT:PCBM) organic solar cells. A nominal 6 nm Au layer was thermally evaporated onto indium tin oxide (ITO) substrates and subsequently annealed at 550 °C for 30 and 60 min before completing the device fabrication. The optical, morphological, and electrical consequences of introducing these annealed Au films were systematically evaluated. Optical measurements revealed a marked enhancement in light absorption: the unannealed Au/P3HT:PCBM film showed a 54% increase at 560 nm, rising to 79% after 60 min of annealing, attributed to localized surface plasmon resonance. In contrast, electrical characterization indicated a decline in overall photovoltaic performance, with all parameters decreasing except for a modest 2% increase in fill factor. Atomic force microscopy further revealed that the actual Au nanofilm thickness was approximately 16 nm—significantly higher than the nominal 6 nm—leading to increased roughness and aggregation. The excessive thickness and roughened morphology of the annealed Au film likely hindered charge transport and reduced exciton generation by scattering and reflecting incident light away from the active layer. These findings highlight the competing effects of Au nanofilms: while they enhance optical absorption, they simultaneously degrade electrical performance. This underscores the importance of carefully optimizing nanofilm thickness and morphology to achieve a balanced interplay between plasmonic enhancement and electronic transport in organic solar cells.
In this study, we presented a straightforward and cost-effective strategy to enhance the photovoltaic performance of poly(3-hexylthiophene-2,5-diyl):[6,6]
1 February 2021 in Journal of Nanoelectronics and Optoelectronics
The effect of the volumetric ratio of the tris(8-hydroxyquinoline) aluminum (Alq3) on its blend with the N,N'-Di [(1-naphthyl)-N,N'-diphenyl]-(1,1'-biphenyl)-4,4'-diamine (NPD) (Alq3:NPD) is investigated and optimized for the UV photodetectors fabrication. The optical and structural properties of Alq3:NPD blend with different volumetric ratios 1:1, 2:1, and 3:1 is studied in the context of the absorbance, transmittance, optical energy gap and XRD patterns. Results show that the absorbance is increased by 11% at A = 260 nm with the increase in the volumetric ratio. In contrast, the optical energy bandgap that is extrapolated from the Tauc’s plot is decreased with the increase in the volumetric ratio, and the 2:1 ratio shows the lowest energy in the UV region. In terms of the XRD investigation, the 2:1 volumetric ratio shows the highest intensity for the crystallinity peak at 36.6°. The fabricated photodetector with a different volumetric ratio of the active layer Alq3:NPD blend shows the best performance with the ratio 2:1.