A liquid-crystalline (LC) semiconductor based on perylene tetracarboxylic bisimide (PTCBI) bearing four 1,1,1,3,3-pentamethyldisiloxane chains was synthesized. This LC PTCBI derivative exhibits ordered columnar phases and the low temperature columnar phase is retained below room temperature. The electron mobility in the ordered columnar phase of this compound at room temperature exceeds 0.1 cm2 V−1 s−1. Moreover, this compound is soluble in various organic solvents, except alcohols, and thin films in which the columnar aggregates are aligned parallel to the substrates are produced by spin-coating. In particular, LC thin films in which the columnar stacks are uniaxially oriented can be produced by a friction transfer method.
In contrast to solid-state organic semiconductors, superstructures can be constructed in liquid-crystalline (LC) phases, using chirality, hybridization with nanofibers, and nanosegregation. Chiral LC molecules form LC phases with helical structures. Gelator molecules self-assemble into fibrous aggregates in LC phases to form nanohybrid materials. Liquid crystal molecules consisting of π-conjugated moieties and incompatible functional parts form nanosegregated LC phases. These nanostructured π-conjugated LC materials have the potential to create new soft matter with unique photonic and electronic functions.
5 March 2014 in Physical Chemistry Chemical Physics
Electron transport characteristics in nanosegregated columnar phases of perylene tetracarboxylic bisimide (PTCBI) derivatives bearing oligosiloxane chains are studied over wide temperature ranges using a time-of-flight (TOF) method. In the ordered columnar phases of the PTCBI derivatives bearing disiloxane chains, the electron mobilities exceed 0.1 cm2 V−1 s−1 at room temperature. In the disordered columnar phase of the PTCBI derivative bearing trisiloxane chains, the electron mobility reaches the order of 10−3 cm2 V−1 s−1 at around room temperature. These electron mobilities are temperature-independent at around room temperature. However, their dependence upon the electric field becomes larger when the temperature is lowered below room temperature; this behavior is described by a hopping transport mechanism. The experimental results are analyzed using a one-dimensional disorder model.
17 December 2014 in Journal of Materials Chemistry C
Ferroelectric liquid-crystalline phenylterthiophene derivatives bearing a decenyl group, disiloxane chain, and cyclotetrasiloxane ring were synthesized. These compounds exhibited a chiral smectic C (SmC*) phase. The spontaneous polarizations of the compounds exceeded 50 nC cm−2. The hole mobilities determined by the time-of-flight method were in the order of 1 × 10−4 cm2 V−1 s−1. The compound with a decenyl group exhibited an anomalous photovoltaic effect in the SmC* phase although the conversion efficiency was lower than 0.01%. Notably, even the compound bearing a bulky cyclotetrasiloxane ring exhibited an enantiotropic SmC* phase.
7 October 2013 in Journal of Materials Chemistry C
Liquid-crystalline perylene tetracarboxylic bisimide derivatives bearing heptamethylcyclotetrasiloxane moieties have been synthesized. Compound 2 bearing four heptamethylcyclotetrasiloxane moieties exhibits a rectangular columnar phase at room temperature. In the columnar phase, the cyclotetrasiloxane rings interdigitate into neighbouring columns and their interaction promotes the formation of the columnar mesomorphic structure. A time-of-flight measurement reveals that the electron mobility in the columnar phase of compound 2 is on the order of 10−2 cm2 V−1 s−1 at room temperature. Compound 2 is soluble in various organic solvents except for alcohol.
A dimer bearing two phenylterthiophene parts linked by a chiral moiety with a minimized molecular volume has been synthesized. This chiral dimer exhibits a chiral nematic phase and its helical structure can be fixed by cooling rapidly. The helical pitch is shorter than the visible light wavelength and the reflection band can be tuned between near ultraviolet and infrared wavelengths by mixing enantiomers of the dimer or changing the temperature. The hole and electron mobilities in the chiral nematic phase are of the order of 10−5 cm2 V−1 s−1. Circularly polarized light emission has been observed in the chiral nematic phase. In the fluidic chiral nematic phase, circularly polarized photoluminescence can be switched to a non-polarized state reversibly by the application of the electric field.