Polymer dielectrics for energy storage applications usually endure high electric field strength. Adjustment of the composition and structure of the dielectric bulk phase to enhance the dielectric breakdown strength has been widely studied. However, the effect of electrode–dielectric interface on the breakdown strength has received little attention, which greatly hinders further development in this field. In this work, an all-organic double-layer dielectric film consisting of poly(vinylidene fluoride) (PVDF) as the matrix and polymethyl methacrylate (PMMA) as the organic nano-interlayer was prepared. By adjusting the electrode–dielectric interface, remarkably improved electric breakdown strength (767.05 MV m−1) and discharged energy density (19.08 J cm−3) were realized concurrently without sacrificing the charge–discharge efficiency. The experimental results and computational simulations reveal that the surface morphology of dielectrics has a great effect on the electric field distribution at the electrode–dielectric interface, and further affects the leakage current and breakdown strength of the dielectric. The PMMA nano-interlayer modifies the surface defects and increases the Young's modulus at the electrode–dielectric interface, leading to the improvement of insulation performance. These findings offer a new perspective to understand the impact of the electrode–dielectric interface on the polymer dielectric breakdown strength. This work provides a novel paradigm for fabricating polymer dielectrics with high breakdown strength for energy storage.
Most commonly used dielectric elastomers (DEs) such as acrylic dielectric elastomers VHB TM 4910 need a high actuation voltage and pre‐stretching to obtain a large actuation strain, and present high mechanical loss caused by viscoelasticity. In this work, we fabricated a new acrylic elastomer by UV curing based on CN9021 and lauryl acrylate. By manipulating crosslinker content, crosslink density changed and physical entanglements of the new material can be affected. Therefore, mechanical properties such as Young's Modulus and mechanical loss of the new material can be controlled, and little change of its glass transition temperature was induced. Results of the actuation test show that the new DE is capable of 9.0% actuation area strain under 11 kV/mm and a good performance under oscillating voltage with different waveforms and frequencies.
1 August 2019 in Journal of Environmental Sciences
Dielectric elastomer (DE) can transfer electrical energy into mechanical energy, who demonstrates significant application potentiality in flexible actuation, sensing, and power generation. However, DE faces the technical bottleneck of high driving electric fields, limiting its practical applications. In this work, an advanced hybridised DE with silicone oil and acrylate was designed to reduce modulus and increase dielectric constant, and realize the characteristic of high driving strain under low electric field. The polysiloxane crosslinking agent with different molecular weight was prepared through the addition reaction between isocyanate and hydroxyl groups, in which dihydroxy‐terminated silicone oil acted as the matrix, 4,4′‐diphenylmethane diisocyanate acted as a chain extender and isocyanoethyl methacrylate acted as a capping agent. In combination with butyl acrylate (BA) to fabricate the new hybridised DE. As a result, the molecular weight of the crosslinker markedly impacts on the hybridised DE's modulus. The introduction of BA enhances the dielectric constant and reduces the modulus. The as‐fabricated PM 2 I‐BA 1 achieves a high actuation sensitivity factor ( β ) of 34.2 and exhibits an actuation strain of 23% under an electric field of 22.5 kV/mm. The linear actuator obtains an output force of 96.3 mN (11 times its own weight) under 12.5 kV/mm.