Characterization and beneficiation studies have been carried out on Brahmagiri placer deposits of Puri, Dist., Odisha. The studies show that this deposit contains potential amount of heavy minerals. The dune sands contain higher heavy minerals than that of beach sand. One of the dune sand samples collected from this deposit shows heavy mineral content of about 29 % also. A composite sand sample is prepared and heavy mineral recovery is studied from this by using gravity table. During recovery of heavy minerals both fresh and sea water are used to see their effect on grade and recovery of concentrate. Sea water rougher gravity table data shows better results than fresh water rougher gravity table. The gravity table study of composite sample shows a yield of 14.8% with a grade of 91.2 % and 93.2 % recovery.
4 June 2013 in High Temperature Materials and Processes
This paper deals with the effect of thermal shock treatment on grindability and grinding characteristics of zircon minerals and the overall energy saving achieved. This attempt is made due to a fine dry grinding of zircon minerals to produce zircon flour is an energy intensive operation. The effect of grinding time on grinding of zircon minerals in a continuously agitated rod mill indicate that the time required is 170 minutes for obtaining 75% of particles passing 45 µm size for natural zircon mineral whereas for thermally treated zircon it is only 100 minutes to achieve the same. Hence, 70 minutes of grinding time is saved. The work index test results show that 13.3% of the total energy can be saved when a sample is preheated to 850 °C and subjected to thermal shock treatment. The effect is due to the development of numerous micro-cracks and fractures in samples subjected to thermal shock.