Recently, fast-setting α-tricalcium-phosphate (TCP) cement was developed for use in the pulp capping process. The aim of this study was to investigate the physical properties and biological effects of α-TCP cement in comparison with mineral trioxide aggregate (MTA).
1 January 2018 in Restorative Dentistry & Endodontics
Background and objectives: This study aimed to investigate the change in bond strength between resin cement and tetragonal zirconia polycrystalline stabilized with 3 to 8 mol% yttrium oxide (Y-TZP) and observe the topographical change of the Y-TZP surface when etched with hydrofluoric acid (HF) solution under different concentration and temperature conditions. Materials and Methods: Non-etched sintered Y-TZP specimens under two different temperature conditions (room temperature and 70–80 °C, respectively), were used as a control, while experimental groups were etched with 5%, 10%, 20%, and 40% HF solutions for 10 min. After zirconia primer and MDP-containing resin cement were applied to the Y-TZP surface, the shear bond strength (SBS) of each experimental group was measured. Results: Under room temperature conditions, the highest SBS value was measured in the 40% HF etching group, representing a significant deviation from the other groups (p < 0.05). In the 70–80 °C tests, the 40% HF etching group also had the highest SBS value, but there was no significant difference when compared to the 20% HF etching group (p > 0.05). From SEM and AFM observations, the HF solution increasingly dissolved the Y-TZP surface grain structure as the concentration and application temperature rose, resulting in high surface roughness and irregularities. Conclusions: Pretreating with either 20% HF solution at 70–80 °C or 40% HF solution at room temperature and 70–80 °C effectively acid etched the Y-TZP surface, resulting in more surface roughness and irregularities. Accounting for the concentration and temperature conditions of the HF solution, using 40% HF solution at room temperature will result in improvements in adhesion between resin cement and Y-TZP.
1 January 2017 in Restorative Dentistry & Endodontics
This study investigated the degree of phase transformation, surface roughness, and bond strength of zirconia immersed for various times in a 40% hydrofluoric acid (HF) solution. Non-etched sintered zirconia specimens were used as the control, while experimental groups were etched with a 40% HF solution for 5, 10, 20, 40, 80, 160 and 320 min. In each of the control and experimental groups, five specimens for X-ray diffraction analysis, four for surface morphology and surface roughness analysis, and ten for bonding strength measurement were used. As a result, the surface roughness of zirconia increased as the application time increased during the 40% HF etching, but the bond strength between zirconia and resin cement did not increase proportionally. The phase transformation from tetragonal to monoclinic also gradually increased with application time.