Ethanol organosolv alfa grass lignins were extracted in the presence of sulfuric acid or Lewis acids (Sc(OTf)3, FeCl3) as catalysts and subjected to a comprehensive structural characterization by solid state 13C NMR, GPC, MALDI-TOF, and ASAP-MS/MS. The impact of the severity of the treatment and of the nature of the acid catalyst on the recovered lignin structure was investigated. The lignins isolated at high severity were highly recondensed and partly composed of regular structures composed of furan-like rings. The alfa (Stipa tenacissima L.) organosolv lignins were used for the preparation of formaldehyde-free adhesives which were characterized by TMA and used for the preparation of particleboard without any addition of synthetic resin. It has been demonstrated for the first time that: (1) the addition of 10% to 30% of organosolv alfa lignin in a tannin-based adhesive improved the adhesive performance; and (2) the conditions of the lignin extraction strongly impact the lignin-based adhesive performances. The highly recondensed lignin extracted with sulfuric acid as a catalyst allowed the production of resins with improved performances. Formulations composed of 50% glyoxalated alfa lignin and 50% of Aleppo Pine tannins yielded good internal bond strength results for the panels (IB = 0.45 MPa) and satisfied relevant international standard specifications for interior-grade panels.
The extraction of condensed tannins from Aleppo pine bark and sumac roots (Brown Rhus tripartitum) was examined in near industrial conditions, using a water medium in the presence of 2% NaHCO3 and 0.5% NaHSO3 at two different temperatures (70 °C and at 100 °C). The tannins extracts were recovered in high yields (~25% of Aleppo pine and ~30% for sumac) with high phenolic contents (>75%). The tannins were characterized by 13C-NMR and MALDI TOF and showed characteristics of procyanidin/prodelphinidin units. The tannins extracted at 100 °C were composed of smaller flavonoid oligomers (DP < 8) compared to those extracted at a lower temperature (DP > 10). Adhesive resin formulations were prepared using Aleppo or sumac tannins and four different cross linkers (hexamine, glutaraldehyde, furfural, and glyoxal). The resins were studied by TMA in bending and tannins-based formaldehyde-free wood particleboards were produced. The panels displayed internal bond strengths > 0.35 MPa with the four hardeners and all of them passed relevant international standard specifications for interior grade panels. The best results were observed with the tannins extracted at 70 °C with furfural as hardener (IB = 0.81 MPa for Aleppo pine and IB = 0.76 MPa for sumac).