Native defects, responsible for the n-type behavior of ZnO are found to be reduced by Mg doping. Zn1−xMgxO nanoparticles synthesized by the conventional coprecipitation route are characterized by XRD, TEM and various spectroscopic techniques like FTIR, XPS, UV-visible, PL, Raman and PAS. Unintentional hydrogen and complex defects in addition to cationic and anionic vacancies (VZn and VO) in ZnO nanoparticles are observed from FTIR. After incorporating Mg, an additional IR mode at 856 cm−1 is observed and attributed to Mg–H. The additional mode contributing excess hydrogen in Mg doped ZnO is further confirmed from XPS. PL and PAS measurements indicate less native defects in Mg doped ZnO because of passivation of defects by excess hydrogen. We conclude that Mg doping not only diminishes the native defects in ZnO, but also could be used as a suitable material for hydrogen storage.
Demonstration of rich sequences of magnetic transitions in 10 and 50 nm particles of CoCr 2 O 4 is shown through dc, ac magnetic measurements, EXAFS and diffused neutron scattering.
CoCr2O4 is a normal spinel where Co occupies the tetrahedral (A) site and Cr occupies the octahedral (B) site; it is important to examine the cation distribution and magnetic properties by substituting a non-magnetic ion like Zn. In this context, we have synthesized pure phase ZnxCo1-xCr2O4 (x = 0.05, 0.1) of crystallite size 10 nm through conventional co-precipitation technique. Fourier transform of Co, Zn, and Cr K-edge spectra obtained from extended X-ray absorption fine structure demonstrates that while Co and Zn prefer the A site, Cr strongly occupies the B site. The paramagnetic to long range ferrimagnetic transition, TC, decreases from 97 K in CoCr2O4 (bulk) to 87.4 K at x = 0.1 with an intermediate TC of 90 K at x = 0.05. The decrease in TC is ascribed to decrease in A-B exchange interaction confirming the preferential occupation of Zn2+ ions towards the A site. The spin-spiral transition, TS, decreases from 27 K in bulk (CoCr2O4) to 24 K at x = 0.1 followed by a spin lock-in transition, TL, observed at 10 K which remains unchanged with increase in Zn concentration. The diffuse neutron scattering in both compositions shows the evidence of long range spiral ordering in contrast to the simultaneous formation of long and short range order in single crystals of CoCr2O4. The decrease in maximum magnetization from 9 to 8 emu/g and an increase in coercivity from 3.2 to 5.2 kOe at 2 K with an increasing Zn concentration from 0.05 to 0.1 have been explained by considering the Yafet-Kittel model.
3 July 2017 in Physical Chemistry Chemical Physics