Thin‐film transistors (TFTs) based on amorphous indium‐gallium‐zinc‐oxide (a‐IGZO) have attracted vast attention for use in organic light‐emitting diode (AMOLED) displays due to their high electron mobility and large current on–off ratio. Although amorphous oxide semiconductors show considerably less threshold voltage (Vth) variation than poly‐silicon, large‐area processing and degradation effects can impede the characteristic parameters of a‐IGZO TFTs, which manifests in an uneven brightness distribution across the display panel. Such Vth variations are usually reduced by additional compensation circuits consisting of TFTs and capacitors. Herein, a new approach to compensate such variabilities is demonstrated: the integration of a programmable ferroelectric (FE) film in the gate stack of the TFT. This simplifies the complexity of the pixel cell and potentially minimizes the need for compensation circuits, which is crucial for transparent displays. To test this new approach, fully integrated FE‐TFTs (i.e., with vias contacting a structured bottom gate electrode from the top) based on a‐IGZO and FE hafnium‐zirconium oxide (HZO) are developed. A single low‐temperature post‐fabrication treatment at 350 °C for 1 h in air is used to simultaneously crystallize the HZO film in the FE phase and to reduce the number of defects in the a‐IGZO channel. The structural and electrical characterizations provide comprehensive guidance for the design of effective FE‐TFT gate stacks and device geometries. An accurate control of the polarization state and linear switching between multiple intermediate states is shown by using programming pulses of various amplitudes and widths. Furthermore, a direct correlation between the channel length and the applied pulse width for programming is observed.
11 June 2018 in ACS Applied Materials & Interfaces
Multi-layer heterostructure oxide semiconductors employing a layer-by-layer deposition of alternating indium oxide and zinc oxide thin films generated via atomic layer deposition (ALD) are investigated for their feasibility into high performance thin film transistors (TFT). The successful deposition of uniform film thickness across the alternating indium oxide and zinc oxide deposition at 200 °C is achieved using trimethyl indium (TMI), diethyl zinc (DEZ) and water as oxidizing agent. The as-prepared polycrystalline material shows a conductive behaviour which upon additional mild annealing between 250–300 °C demonstrates a high TFT device performance. In addition, insights into the dependency of the defect passivation gradient within the multilayer upon thermal annealing of the oxide stack are presented. Studies towards an optimised film thickness result in a high device performance in enhancement mode with a saturation field-effect mobility (μsat.) of 6.5 cm2 V−1 s−1 and an on/off ratio (Ion/off) of 4.6 × 107 using a deliberately large width to length channel ratio (W/L = 500). The TFT performance turned out to be dependent on the position of the individual oxide layers within the stack and the number of heterostructure stacks. These findings on the influence of semiconductor stack formation allow for a better understanding on the formation of the active semiconductor channel and serve towards the applicability of ALD based heterostructure metal oxide semiconductors in next generation electronics.
13 June 2017 in ACS Applied Materials & Interfaces
Amorphous aluminium oxide thin films are accessible by a molecular single source precursor approach employing the coordination compound tris[(diethyl-2-nitromalonato)]aluminium(III) (Al-DEM-NO2). The precursor decomposes by thermal combustion under oxygen without the need of an additional additive into amorphous aluminium oxide films at 350 °C with a very low surface roughness of about 0.3 nm. Solution processing of the precursor results in the formation of smooth, dense and crack-free films, which are converted into amorphous AlxOy thin films after further calcination. Amorphous AlxOy thin films integrated within a capacitor device exhibit dielectric behavior in the temperature range between 200 and 350 °C, with areal capacity values between 41 and 86 nF cm−2 and leakage current densities ranging from 1.7 × 10−7 to 8.9 × 10−10 A cm−2 (at 1 MV cm−1) whereas breakdown voltages increase from 1.82 to 2.79 MV cm−1 in the temperature regime from 200 to 350 °C. The increase in performance at higher temperatures can be attributed to the stepwise conversion of the intermediate aluminium oxo–hydroxy species into aluminium oxide which is confirmed by X-ray photoelectron spectroscopy (XPS).