Jan Allen

Dr. Jan Allen

US Army Research Laboratory
orcid

Research Focus & Metrics

Academic Career Length

26Years (2001-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 May 2012 in Journal of Power Sources
Verified
Journal Article
Closed access
Jan AllenJan Allen
Jan Allen
JWJ. Wolfenstine
J. Wolfenstine
ERE. Rangasamy
E. Rangasamy
JSJ. Sakamoto
J. Sakamoto

25 January 2018 in Journal of the Electrochemical Society
Verified
Journal Article
Open access
PDF file
TJT. Richard Jow
T. Richard Jow
SDSamuel A. Delp
Samuel A. Delp
Jan AllenJan Allen
Jan Allen
JJJohn-Paul Jones
John-Paul Jones
MSMarshall C. Smart
Marshall C. Smart
Understanding the factors limiting Li+ charge transfer kinetics in Li-ion batteries is essential in improving the rate performance, especially at lower temperatures. The Li+ charge transfer process involved in the lithium intercalation of graphite anode includes the step of de-solvation of the solvated Li+ in the liquid electrolyte and the step of transport of Li+ in the preformed solid electrolyte interphase (SEI) on electrodes until the Li+ accepts an electron at the electrode and becomes a Li in the electrode. Whether the de-solvation process or the Li+ transport through the SEI is a limiting step depends on the nature of the interphases at the electrode and electrolyte interfaces. Several examples involving the electrode materials such as graphite, lithium titanate (LTO), lithium iron phosphate (LFP), lithium nickel cobalt aluminum oxide (NCA) and solid Li+ conductor such as lithium lanthanum titanate or Li-Al-Ti-phosphate are reviewed and discussed to clarify the conditions at which either the de-solvation or the transport of Li+ in SEI is dominating and how the electrolyte components affect the activation energy of Li+ charge transfer kinetics. How the electrolyte additives impact the Li+ charge transfer kinetics at both the anode and the cathode has been examined at the same time in 3-electrode full cells. The resulting impact on Li+ charge transfer resistance, Rct, and activation energy, Ea, at both electrodes are reported and discussed.

27 January 2017 in ACS Energy Letters
Verified
Journal Article
Closed access
TTTravis Thompson
Travis Thompson
SYSeungho Yu
Seungho Yu
LWLogan Williams
Logan Williams
RSRobert D. Schmidt
Robert D. Schmidt
RGRegina Garcia-Mendez
Regina Garcia-Mendez
JSJeff Sakamoto
Jeff Sakamoto

24 June 2014 in Journal of Materials Chemistry A
Verified
Journal Article
Closed access
PDF file
TTTravis Thompson
Travis Thompson
JWJeff Wolfenstine
Jeff Wolfenstine
Jan AllenJan Allen
Jan Allen
MJMichelle Johannes
Michelle Johannes
AHAshfia Huq
Ashfia Huq
JSJeff Sakamoto
Jeff Sakamoto
Li7La3Zr2O12 (LLZO) garnet is attracting interest as a promising Li-ion solid electrolyte. LLZO exists in a tetragonal and cubic polymorph where the cubic phase exhibits ∼2 orders of magnitude higher Li-ion conduction. It has been suggested that a critical Li vacancy concentration (0.4–0.5 atoms per formula unit) is required to stabilize the cubic polymorph of Li7La3Zr2O12. This has been confirmed experimentally for Al3+ doping on the Li+ site. Substitution of M5+ (M = Ta, Nb) for Zr4+ is an alternative means to create Li vacancies and should have the same critical Li vacancy concentration, nevertheless, subcritically doped compositions (0.25 moles of Li vacancies per formula unit) have been reported as cubic. Adventitious Al, from alumina crucibles, was likely present in these studies that could have acted as a second dopant to introduce vacancies. In this work, Al-free subcritically doped (Li6.75La3Zr1.75Ta0.25O12) and critically doped (Li6.5La3Zr1.5Ta0.5O12) compositions are investigated. X-ray diffraction indicates that both compositions are cubic. However, upon further materials characterization, including SEM analysis, Raman spectroscopy, Electrochemical Impedance Spectroscopy, and neutron diffraction it is evident that the subcritically doped composition is a mixture of cubic and tetragonal phases. The results of this study confirm that 0.4–0.5 Li vacancies per formula unit are required to stabilize the cubic polymorph of LLZO.

1 January 2002 in Journal of the Electrochemical Society
Verified
Journal Article
Closed access
PDF file
KXKang Xu
Kang Xu
MDMichael S. Ding
Michael S. Ding
Sheng S. ZhangSheng S. Zhang
Sheng S. Zhang
Jan AllenJan Allen
Jan Allen
TJT. Richard Jow
T. Richard Jow
Using alkyl phosphates and a cyclophosphazene as cosolvents, the possibility of formulating a nonflammable electrolyte for lithium-ion batteries was explored. The emphasis was placed on determining the impact of these flame-retarding additives on the performance of the electrolyte. It was found that although the cosolvents at high contents <mml:math display="inline"><mml:mo stretchy="false">(</mml:mo><mml:mo>></mml:mo><mml:mn>10</mml:mn><mml:mo>%</mml:mo><mml:mo stretchy="false">)</mml:mo></mml:math>(>10%) effectively suppress the flammability of the electrolyte, their flame-retarding effectiveness is still insufficient to render the electrolytes completely nonflammable. Furthermore, such reduction in electrolyte flammability is always realized at the expense of performance; electrochemical instability of phosphates results in severe capacity fading, while high viscosity of these cosolvents reduces both capacity utilization and power. © 2002 The Electrochemical Society. All rights reserved.

1 January 2001 in Electrochemical and Solid-State Letters
Verified
Journal Article
Closed access
PDF file
Sheng S. ZhangSheng S. Zhang
Sheng S. Zhang
MDMichael S. Ding
Michael S. Ding
KXKang Xu
Kang Xu
Jan AllenJan Allen
Jan Allen
TJT. Richard Jow
T. Richard Jow
Using ac impedance, we studied the formation process of solid electrolyte interface (SEI) film on graphite electrode during initial cycles. Results show that the SEI formation takes place through two major stages. The first stage takes place at voltages above 0.25 V (before lithiation of graphite), during which a loose and highly resistive film is formed. The second stage occurs at a narrow voltage range of 0.25-0.04 V, which proceeds simultaneously with lithiation of graphite electrode. In the second stage, a stable, compact, and highly conductive SEI film is produced. © 2001 The Electrochemical Society. All rights reserved.