In the preparation of an Al-Ti-C grain refiner under an ultrasonic field, the mechanism of the wetting behaviour between Al and C was systematically investigated. The results demonstrated that the wetting behaviour was mainly dependent on the wetting of the Al melt on graphite under the ultrasonic field (physical wetting) and the formation and mass transfer of TiC (reactive wetting). The diffusion of Ti atoms and their adsorption around the graphite could contribute to the wetting of Al-C. TiC particles were formed under the high temperature caused by the cavitation effect, and they detached from the interface due to the sound pressure, which resulted in consistently sufficient contact on the wetting interface. Moreover, the wetting and spreading behaviour of the Al melt on graphite under an ultrasonic field were numerically simulated, strongly manifesting that the ultrasonic field could facilitate the wetting of the Al-C interface.
Al and Al-5Ti alloys were manufactured by an ultrasonic casting method with a new device, and their ultrasonic cavitation erosion behaviors of Al and Al-5Ti alloys in the distilled water were clarified. The damage mechanism was analyzed by macro photograph, scanning electronic micrograph and three-dimensional morphology, and the results demonstrate that Al-5Ti alloys have better cavitation erosion resistance than Al in terms of the mass loss and the surface damage. The deformation mechanism of Al and Al-5Ti alloys under cavitation erosion is mainly dislocation slip, and the Al3Ti phase enhances the cavitation erosion resistance of Al-5Ti alloys. In addition, the maximum depth of cavitation pits in the Al-5Ti sample is less than that in the Al sample for 31.3%.
Two kinds of Ti-alloys, i.e., Al–5Ti and Al–10Ti alloys, were manufactured in this study, and their ultrasonic cavitation erosion behaviors in 3.5 wt.% NaCl solution were evaluated by the cumulative mass loss, scanning electronic micrograph, and three-dimensional morphology. The results show that mass loss and surface damage of the Al, Al–5Ti, and Al–10Ti alloys obviously increased with the increasing cavitation erosion time. Compared with the pure Al, the cavitation resistance of the Al–5Ti and Al–10Ti alloys was improved because of the presence of the TiAl3 phase. In addition, the synergistic effect between cavitation and corrosion of the Al–Ti alloy in 3.5 wt.% NaCl solution was studied according to the polarization curve of the moving electrode. The mass loss caused by the synergistic effect between cavitation erosion and corrosion accounted for a large percentage, 23.59%, indicating that corrosion has a critical impact on the cavitation erosion of the Al–Ti alloys. Compared with corrosion promoted by cavitation erosion, the cavitation erosion promoted by corrosion had a larger promoting effect.
10 February 2024 in Metals and Materials International
Approaches of optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction, electron backscattered diffraction (EBSD), transmission electron microscopy (TEM) and mechanical property testing have been used to study the microstructure and mechanical properties of Mg-6.1Zn-0.7Zr alloys before and after equal channel angular pressing (ECAP) investigated in detail using. The study demonstrates that the microstructure comprises of fine-grained equiaxed dynamic recrystallization. The size of various grains is in the range 2.3-5.2 μm along the boundaries of unrecrystallized grains after 6 passes of ECAP. Meanwhile, the Mg-Zn and Mg-Zn-Zr compounds gradually crush into fine dispersed particles and the dislocation density increases. With increase of pass the average (0001) basal slip Schmid factor gradually increases to 0.41. The strength and ductility have improved with increasing of ECAP pass. Notably, after 6 passes, due to decrease of grain size and the strengthening effects of fragmentized secondary phase particles, the ultimate tensile strength increases to 260 MPa, and the elongation at break exceeds 28.6%.
A key technical problem in the preparation of Al-Ti-C grain refiner and other composite materials is the poor wetting of the Al-C interface, which greatly restricts the development of the preparation technology of related composite materials. In view of this scientific challenge, a novel ultrasonic field wetting angle measuring instrument has been designed to research the wetting behavior of the liquid–solid interface and ensure that preparation conditions are optimized. The dimensional parameters of the ultrasonic transducer and the horn in the novel ultrasonic wetting angle measuring instrument have been designed by theoretical calculation, and the modal analysis was performed for the ultrasonic horn using the functions of displacement and time. Modal analysis was utilized to optimize the dimension of the ultrasonic horn, and the natural frequency of the longitudinal vibration of the horn was reduced from 22,130 Hz to 22,013 Hz, resulting in an error rate between the actual value (22,013 Hz) and the design value (20 kHz) of less than 1%. In addition, the influence of different transition arc radiuses on the maximum stress of the optimized ultrasonic horn was analyzed.