In this study, the compression molding process parameters for the development of silk fiber-reinforced polypropylene composites was optimized using Box–Behnken experimental Design with response surface methodology. The trimmed silk fibers from shuttleless loom silk selvedge waste were used as reinforcement in polypropylene fiber matrix. The process parameters of compression molding such as temperature (165–185℃), time (7–15 min) and pressure (35–45 bar) were optimized with respect to the mechanical properties of the silk fiber-reinforced polypropylene composite. The optimum parameters for better mechanical properties were found to be temperature, 180℃; time, 7 min, and pressure, 35 bar in compression molding. The optimised level of parameters has shown good response to the predicted model.
17 November 2013 in Journal of Industrial Textiles
The intimately mixed natural protein fiber hybrid composites in three different fiber concentrations (70:30, 50:50 and 30:70) and two different fiber orientations (parallel laid and cross laid) are produced using silk and wool fibers with polypropylene fibers as matrix material. The composites are fabricated using compression molding technique with optimized process conditions. The effects of fiber content and fiber orientation on mechanical, thermal conductivity and water absorption property are studied. Scanning electron microscope is used to examine the fracture morphology of the composites. The study reveals that the fiber content strongly influences the mechanical, thermal conductivity and water absorption property of the resultant composite. But the fiber orientation shows significant effect only on water absorption property of the composites. It does not show any significant difference in mechanical and thermal conductivity properties of intimately mixed silk/wool hybrid fiber composites.
1 September 2014 in Journal of Engineered Fibers and Fabrics
The present study focused optimizing the process parameters of compression molding with respect to mechanical properties for fabrication of wool fiber-reinforced polypropylene composites. An experiment was designed using the Box-Behnken method with three levels and three variables using temperature, time, and pressure, as independent variables and tensile, flexural, and impact strengths as dependent variables. The process conditions were optimized using response surface methodology with the Box-Behnken experimental design. Regression equations were obtained to analyze tensile strength, flexural strength, and impact strength and the optimum process parameters were identified. The results show that the optimum conditions for compression molding are 176°C, 7 min, and 35 bar.
19 July 2023 in Biomass Conversion and Biorefinery
This article emphasizes the optimization of the retrieval of silk fibers from silk selvedge waste in a hard waste opening machine. It also highlights the characterization of composites developed from retrieved silk fibers with a polypropylene matrix in a compression molding machine. The machine conditions of the hard waste opener, such as the licker-in speed, cylinder speed, and setting between feed roller to licker-in, were optimized with respect to the fiber staple length using the Box-Behnken experimental design with response surface methodology. The optimum conditions for the fiber staple length were found to be licker-in speed, 550 r/min; cylinder speed, 280 r/min; and setting between feed roller to licker-in, 0.01 inch. Composites were developed using the silk fibers retrived at optimum conditions with polypropylene resin in compression molding at three different fiber loadings, namely 40, 50, and 60 weight % of silk fibers. The influece of silk fiber loading on the mechanical and thermal properties of the composites were studied and compared to pure PP composite. It is observed from the results that the composite with 50 weight % of silk fiber loading has shown greater mechanical properties. Furthermore, the incorporation of silk fibers in the polypropylene matrix has shown an improvement in the mechanical properties of 71.6 %, 76.66 %, 69.73 %, 67.97 %, and 58.45 % for tensile strength, tensile modulus, flexural strength, flexural modulus, and impact strength, respectively, in the composites when compared to pure polypropylene composite. The Differential Scanning Calorimetry analysis has also shown an increase in the degradation temperature of 8°C in the silk fiber-reinforced composite.