In this work, an equiatomic TiNbTaMoZr-based high-entropy alloy (HEA) has been developed by a powder metallurgy route, which consists of a process of combined one-step low-temperature mechanical milling starting from the transition metals as raw materials and a subsequent pressureless sintering. In this way, the optimized synthesized specimen, after 10 h of milling time, showed two different body-centered cubic (bcc) TiNbTaMoZr alloys, which, after sintering at 1450 °C, 1 h of dwell time and a heating and cooling rate of 5 °C min−1, it remained formed as two bcc TiNbTaMoZr-based HEAs. This material, with micrometric and equiaxed particles, and with homogeneously distributed phases, presented a Young’s modulus that was significantly higher (5.8 GPa) and lower (62.1 GPa) than that of the usual commercially pure (cp) Ti and Ti6Al4V alloy used for bone-replacement implants. It also presented similar values to those of the HEAs developed for the same purpose. These interesting properties would enable this TiNbTaMoZr-based HEA to be used as a potential biomaterial for bulk or porous bone implants with high hardness and low Young´s modulus, thereby preventing the appearance of stress-shielding phenomena.
MAX phases are an advanced class of ceramics based on ternary carbides or nitrides that combine some of the ceramic and metallic properties, which make them potential candidate materials for many engineering applications under severe conditions. The present work reports the successful synthesis of nearly single bulk Ti2AlN MAX phase (>98% purity) through solid-state reaction and from a Ti and AlN powder mixture in a molar ratio of 2:1 as starting materials. The mixture of Ti and AlN powders was subjected to reactive spark plasma sintering (SPS) under 30 MPa at 1200 °C and 1300 °C for 10 min in a vacuum atmosphere. It was found that the massive formation of Al2O3 particles at the grain boundaries during sintering inhibits the development of the Ti2AlN MAX phase in the outer zone of the samples. The effect of sintering temperature on the microstructure and mechanical properties of the Ti2AlN MAX phase was investigated and discussed.
In this work, the mechanical and bio-functional behavior of a TiNbTa alloy is evaluated as a potential prosthetic biomaterial used for cortical bone replacement. The results are compared with the reference Ti c.p. used as biomaterials for bone-replacement implants. The estimated mechanical behavior for TiNbTa foams was also compared with the experimental Ti c.p. foams fabricated by the authors in previous studies. A TiNbTa alloy with a 20–30% porosity could be a candidate for the replacement of cortical bone, while levels of 80% would allow the manufacture of implants for the replacement of trabecular bone tissue. Regarding biocompatibility, in vitro TiNbTa, cellular responses (osteoblast adhesion and proliferation) were compared with cell growth in Ti c.p. samples. Cell adhesion (presence of filopodia) and propagation were promoted. The TiNbTa samples had a bioactive response similar to that of Ti c.p. However, TiNbTa samples show a better balance of bio-functional behavior (promoting osseointegration) and biomechanical behavior (solving the stress-shielding phenomenon and guaranteeing mechanical resistance).
The influence of the mechanical activation process and sintering atmosphere on the microstructure and mechanical properties of bulk Ti2AlN has been investigated. The mixture of Ti and AlN powders was prepared in a 1:2 molar ratio, and a part of this powder mixture was subjected to a mechanical activation process under an argon atmosphere for 10 h using agate jars and balls as milling media. Then, the sintering and production of the Ti2AlN MAX phase were carried out by Spark Plasma Sintering under 30 MPa with vacuum or nitrogen atmospheres and at 1200 °C for 10 min. The crystal structure and microstructure of consolidated samples were characterized by X-ray Diffraction, Scanning Electron Microscopy, and Energy Dispersive X-ray Spectroscopy. The X-ray diffraction patterns were fitted using the Rietveld refinement for phase quantification and determined their most critical microstructural parameters. It was determined that by using nitrogen as a sintering atmosphere, Ti4AlN3 MAX phase and TiN were increased at the expense of the Ti2AlN. In the samples prepared from the activated powders, secondary phases like Ti5Si3 and Al2O3 were formed. However, the higher densification level presented in the sample produced by using both nitrogen atmosphere and MAP powder mixture is remarkable. Moreover, the high-purity Ti2AlN zone of the MAX-1200 presented a hardness of 4.3 GPa, and the rest of the samples exhibited slightly smaller hardness values (4.1, 4.0, and 4.2 GPa, respectively) which are matched with the higher porosity observed on the SEM images.
In this work, a blend of Ti, Nb, and Mn powders, with a nominal composition of 15 wt.% of Mn, and balanced Ti and Nb wt.%, was selected to be mechanically alloyed by the following two alternative high-energy milling devices: a vibratory 8000D mixer/mill® and a PM400 Retsch® planetary ball mill. Two ball-to-powder ratio (BPR) conditions (10:1 and 20:1) were applied, to study the evolution of the synthesized phases under each of the two mechanical alloying conditions. The main findings observed include the following: (1) the sequence conversion evolved from raw elements to a transitory bcc-TiNbMn alloy, and subsequently to an fcc-TiNb15Mn alloy, independent of the milling conditions; (2) the total full conversion to the fcc-TiNb15Mn alloy was only reached by the planetary mill at a minimum of 12 h of milling time, for either of the BPR employed; (3) the planetary mill produced a non-negligible Fe contamination from the milling media, when the highest BPR and milling time were applied; and (4) the final fcc-TiNb15Mn alloy synthesized presents a nanocrystalline nature and a partial degree of amorphization.