Pure NiO nanoparticles were subjected to isochronal thermal treatments in open air from 100 to 1000°C. X-ray diffraction (XRD) patterns indicate that all annealed samples exhibit a single phase of face-centered cubic (FCC) crystalline structure, obvious grain growth occurs only above 400°C and the average crystallite size increases from 20 to 80 nm. X-ray photoelectron spectroscopy (XPS) shows that only very few amount of Ni3 + and no impurity element have been found in the annealed samples. Positron annihilation measurements reveal that large number of Ni-vacancy defects exist in the grain surface region. These surface defects begin to recover after annealing above 400°C, and most of them are removed at 1000°C. Room temperature ferromagnetism is obviously observed for the samples annealed at 100 and 400°C. The saturation magnetization gradually decreases with the increase of the annealing temperature, and it almost disappears at 800 and 1000°C. The disappearance of ferromagnetism shows good coincidence with the recovery of Ni-vacancies. Our results suggest that the anomalous ferromagnetic behavior in NiO nanoparticles might be due to the surface Ni-vacancy defects instead of grain size effects.
In this study, polycrystalline SnSe was synthesized via a rapid, cost-effective, and large-scale synthesis route. The obtained SnSe powders were pressed into pellets via spark plasma sintering (SPS) at different temperatures. Powder X-ray diffraction (XRD) and field-emission scanning electron microscopy (FESEM) were used to characterize the crystal structures and morphology of the SnSe samples. The XRD results indicate that the orientation factors increase monotonously with the increase of sintering temperature. The FESEM images show that sintering temperatures have no obvious influence on the particle size. Positron annihilation measurements indicate that vacancy defects exist in all the sintered SnSe samples, and they recover gradually with increasing sintering temperatures. These vacancy defects are responsible for the lower lattice thermal conductivity in samples sintered at lower temperatures. The electrical conductivity, power factor, thermal conductivity, and figure of merit ZT show nearly the same variation trend, which increases initially with the increasing sintering temperature up to 550 C then decreases with further increase of the sintering temperature, which is possibly due to slight oxidation of SnSe. A maximum ZT value of 0.47 at 430 C was achieved for the 550 C sintered sample, which is higher than those reported for undoped polycrystalline SnSe around this temperature. Thus, we provide a simple, energy-saving, and effective method to synthesize polycrystalline SnSe in large quantities, and SPS is an effective method to optimize thermoelectric performance.
CuO/ZnO nanocomposites with 4 at. % CuO were annealed in air at various temperatures between 100 and 1200 °C to produce Cu-doped ZnO nanocrystals. X-ray diffraction shows that a CuO phase can be observed in the CuO/ZnO nanocomposites annealed at different temperatures, and the Cu-doped ZnO nanocrystals are identified to be of wurtzite structure. The main peak (101) appears at slightly lower diffraction angles with increasing annealing temperature from 400 up to 1200 °C, which confirms the successful doping of Cu into the ZnO lattice above 400 °C. Scanning electron microscopy indicates that most particles in the CuO/ZnO nanocomposites are isolated when annealing at 100–400 °C, but these particles have a tendency to form clusters or aggregates as the annealing temperature increases from 700 to 1000 °C. Positron annihilation measurements reveal a large number of vacancy defects in the interface region of the nanocomposites, and they are gradually recovered with increasing annealing temperature up to 1000 °C. Room-temperature ferromagnetism can be observed in the CuO/ZnO nanocomposites, and the magnetization decreases continuously with increasing annealing temperature. However, there may be several different origins of ferromagnetism in the CuO/ZnO nanocomposites. At low annealing temperatures, the ferromagnetism originates from the CuO nanograins, and the ferromagnetism of CuO nanograins decreases with an increase in the grain size after subsequent higher temperature annealing, which leads to the weakening of ferromagnetism in the CuO/ZnO nanocomposites. After annealing from 400 to 1000 °C, the ferromagnetism gradually vanishes. The ferromagnetism is probably induced by Cu substitution but is mediated by vacancy defects in the CuO/ZnO nanocomposites. The disappearance of ferromagnetism coincides well with the recovery of vacancy defects. It can be inferred that the ferromagnetism is mediated by vacancy defects that are distributed in the interface region.
The transmittance and the defect mode (DM) are investigated in a one-dimensional superconducting photonic crystal (PC). The structure is composed of periodically stacked SD/DS pairs with a strict central symmetry, where S and D denote superconductor and dielectric layers, respectively. A sharp and narrow DM emerges at the center of the photonic bandgap. Transmission peak degeneracy can be observed by increasing the period number. With this fractal-like behavior, the transmittance is highly sensitive to external stimuli. The DM wavelength λc linearly blue-shifts with the hydrostatic pressure, and monotonically red-shifts with the temperature. While increasing the incident angle, λc bule-shifts first smoothly and then sharply. Notably, enhanced tunability is achieved under low pressures, elevated temperatures, and large incidence angles, suggesting superior modulation capabilities. High pressure sensitivity of the DM wavelength, up to 128nm/GPa, is achieved with low deformations. Moreover, the DM maintains near-perfect transmittance unless the temperature is higher than the critical temperature of the superconductor. These findings highlight the potential of such defect-engineered superconducting PCs for high-performance optical sensing applications.