Tin-doped indium oxide (ITO) deposited by vacuum process with excellent optical and electrical properties have been generally used as transparent conductive oxide thin films. In view of high cost and difficulty in recycles for vacuum process, zinc oxide films synthesized by wet chemical process are therefore regarded as a more suitable candidate to replace ITO. In this work, sol-gel method was used to synthesize transparent aluminum-doped zinc oxide (ZnO:Al, AZO) with 450nm thickness for large scale production of CIGS solar cell. The experimental parameters included different solvents, the propylene glycol methyl ether (PGME) to replace the usually used solvent ethylene glycol monomethyl ether (EGME) which is toxic, the amount of Al dopant (ranged from 0 to 2 at%), and various annealing temperatures. The structure, electrical and optical properties of AZO thin films are investigated by a field emission scanning electron microscope (FE-SEM), transmission electron microscope (TEM), X-ray diffractometer (XRD), four-point probe (FPP) and ultraviolet visible light spectroscope (UV-VIS) etc. The experimental results showed that the AZO films were wurtzite crystalline with c-axis preferred orientation and had > 85% transmittance and lower electrical resistivity after annealed in N2 atmosphere. The optimum AZO samples had low electrical resistivity of 1.94¥10-2 Ω-cm, which were synthesized with PGME solvent, 1 at% Al-doping and annealed at 600°C in N2 atmosphere and 500°C in 95 N2/5 H2 atmosphere for one hour, separately
In this work, nickel thin films were deposited on texture silicon by electroless plated deposition. The electroless-deposited Ni layers were characterized by scanning electron microscopy (SEM), transmission electron microscopy (TEM), energy dispersive x-ray spectroscopy (EDS), X-ray diffraction analysis (XRD), and sheet resistance measurement. The results indicate that the dominant phase was Ni2Si and NiSi in samples annealed at 300–800 °C. Sheet resistance values were found to correlate well with the surface morphology obtained by SEM and the results of XRD diffraction. The Cu/Ni contact system was used to fabricate solar cells by using two different activating baths. The open circuit voltage (Voc) of the Cu/Ni samples, before and after annealing, was measured under air mass (AM) 1.5 conditions to determine solar cell properties. The results show that open circuit voltage of a solar cell can be enhanced when the activation solution incorporated hydrofluoric acid (HF). This is mainly attributed to the native silicon oxide layer that can be decreased and/or removed by HF with the corresponding reduction of series resistance.
10 July 2020 in Journal of Materials Science: Materials in Electronics
This study investigated the use of a pure copper seed layer to improve the adhesion strength and reduce the residual stress of electroplated copper films for heterojunction technology in crystalline solar cells. The experiment involved depositing a copper seed layer and an indium tin oxide (ITO) layer on textured silicon using sputtering. This resulted in the formation of a Cu(s)/ITO/Si structure. Following this step, a 10 µm thick copper layer was electroplated onto the Cu(s)/ITO/Si structure. Various characterization techniques were employed to evaluate the electroplated copper films’ microstructures, residual stress, and adhesion strength. The microstructures of the films were examined using a scanning transmission electron microscope (STEM), revealing a twin structure with a grain size of approximately 1 µm. The residual stresses of the as-deposited and annealed samples were measured using an X-ray diffractometer (XRD), yielding values of 76.4 MPa and 49.1 MPa, respectively. The as-deposited sample exhibited higher tension compared to the annealed sample. To assess the adhesion strength of the electroplated copper films, peel-off tests were conducted at a 90° angle with a constant speed of 30 mm/min. The peel force, measured in units of N/mm, was similar for both the as-deposited and annealed samples. Specifically, the peel force for electroplating copper on the copper seed layer on the ITO was determined to be 2.6 N/mm for the maximum value and 2.25 N/mm for the average value. This study demonstrated that using a pure copper seed layer during electroplating can improve adhesion strength and reduce residual stress in copper films for heterojunction technology in crystalline solar cells. These findings contribute to the development of more reliable and efficient solar-cell-manufacturing processes.
Various structures of Cu (50 nm)/Ru (2 nm)/MgO (0.5–3 nm)/Ta (2 nm)/Si were prepared by sputtering and electroplating techniques, in which the ultra-thin trilayer of Ru (2 nm)/MgO (0.5–3 nm)/Ta (2 nm) is used as the diffusion barrier against the interdiffusion between Cu film and Si substrate. The various structures of Cu/Ru/MgO/Ta/Si were characterized by four-point probes for their sheet resistances, by X-ray diffractometers for their crystal structures, by scanning electron microscopes for their surface morphologies, and by transmission electron microscopes for their cross-section and high resolution views. The results showed that the ultra-thin tri-layer of Ru (2 nm)/MgO (0.5–3 nm)/Ta (2 nm) is an effective diffusion barrier against the interdiffusion between Cu film and Si substrate. The MgO, and Ta layers as deposited are amorphous. The mechanism for the failure of the diffusion barrier is that the Ru layer first became discontinuous at a high temperature and the Ta layer sequentially become discontinuous at a higher temperature, the Cu atoms then diffuse through the MgO layer and to the substrate at the discontinuities, and the Cu3Si phases finally form. The maximum temperature at which the structures of Cu (50 nm)/Ru (2 nm)/MgO (0.5–3 nm)/Ta (2 nm)/Si are annealed and still have low sheet resistance is from 550 to 750 °C for the annealing time of 5 min and from 500 to 700 °C for the annealing time of 30 min.
1 April 2009 in International Journal of Minerals, Metallurgy and Materials