The microstructures of an electron beam melted (EBM) nickel-based superalloy (Alloy 718) were comprehensively investigated in as-built and post-treated conditions, with particular focus individually on the contour (outer periphery) and hatch (core) regions of the build. The hatch region exhibited columnar grains with strong 〈001〉 texture in the build direction, while the contour region had a mix of columnar and equiaxed grains, with no preferred crystallographic texture. Both regions exhibited nearly identical hardness and carbide content. However, the contour region showed a higher number density of fine carbides compared to the hatch. The as-built material was subjected to two distinct post-treatments: (1) hot isostatic pressing (HIP) and (2) HIP plus heat treatment (HIP + HT), with the latter carried out as a single cycle inside the HIP vessel. Both post-treatments resulted in nearly an order of magnitude decrease in defect content in hatch and contour regions. HIP + HT led to grain coarsening in the contour, but did not alter the microstructure in the hatch region. Different factors that may be responsible for grain growth, such as grain size, grain orientation, grain boundary curvature and secondary phase particles, are discussed. The differences in carbide sizes in the hatch and contour regions appeared to decrease after post-treatment. After HIP + HT, similar higher hardness was observed in both the hatch and contour regions compared to the as-built material.
Continuous alumina fiber exhibits excellent mechanical properties owing to its dense microstructure with fine grains. In this study, alumina fiber was prepared by the sol–gel method using iron sol as a nucleating agent. It was proposed that the α-Al2O3 grain size be adjusted based on the modification of colloidal particle size. The effect of holding temperature and reaction material ratio on the iron colloidal particle size was studied. The microstructure of alumina fiber was characterized by scanning electron microscopy (SEM). The experiment results indicated that iron colloidal particle size increases with the holding temperature and the NH4HCO3/Fe(NO3)3·9H2O ratio. The alumina fiber with uniform nano α-Al2O3 grains was obtained by calcination at 1400 °C for 5 min. The mean grain size tends to rise with the mean colloidal particle size. Using the iron sol as a nucleating agent, the fiber with a mean grain size of 22.5 nm could be formed. The tensile strength of fibers increased with the decrease of grain size.
18 June 2021 in Journal of Sol-Gel Science and Technology