This study evaluated the effect of thickness and photo-polymerization distance on flexure strength of two bulk fill resin composites. In total, 96 rectangular-shaped resin composite bars were divided into eight experimental groups (n = 12/group) according to the three experimental factors; Factor 1: Material (X-tra fil and Admira Fusion X-tra), Factor 2: Thickness (2 mm and 4 mm) and Factor 3: photo-polymerization distance (2 mm and 8 mm). The bars were prepared with fixed 2 mm width and 2 mm length but differed in thickness (2 mm or 4 mm). The bars were light cured either at 2 mm or 8 mm distances. Flexure strength test was run at a crosshead speed of 0.5 mm/min. Data were analyzed using 3-Way ANOVA/Student t-test. Methacrylate-based resin composite exhibited significant higher flexure strength (p < 0.001). At 2 mm distance, there was no significant difference between 2 mm and 4 mm thicknesses for X-tra fil and Admira Fusion X-tra (p = 0.726 and p = 0.486, respectively). At 8 mm distance, both materials showed significantly higher flexure strength with 4 mm thickness compared to 2 mm thickness (p ˂ 0.001). Only X-tra fil with 2 mm thickness had no statistically significant difference on the flexure strength at 2 mm and 8 mm distances (p = 0.437). X-tra fil in 2 mm thickness cured at 8 mm distance and Admira Fusion X-tra in 4 mm thickness cured at 2 mm distance revealed the highest reliability. Methacrylate-based resin composite tested in this study had superior flexure strength compared to ormocer-based resin composite, regardless of the increment thickness and photo-polymerization distance.
21 December 2020 in Journal of Adhesion Science and Technology
This study evaluated the effect of pre-heating a dual-polymerized adhesive and a dual-polymerized core build-up resin composite on their dentin micro-shear bond strength (µSBS), degree of conversion (DC%) and ultimate tensile strength (UTS). For µSBS, 45 human molars were divided into 9 groups (n = 5) according to two factors: (1) Adhesive temperature (25 °C/32 °C/40 °C) and 2- Resin composite temperature (25 °C/32 °C/40 °C). Dual-polymerized adhesive (Futurabond U/FBU) was applied over occlusal dentin at each temperature following the manufacturer’s instructions. Four dual-polymerized composites (Rebilda DC/RDC, VOCO) micro-cylinders (1.2 mm diameter × 1 mm height) were built-up over each dentin disc, after being pre-heated at each temperature. After storage (48 h/37 °C), µSBS testing was run at a crosshead speed of 1 mm/min. DC% of FBU/RDC was evaluated at each temperature after 48 h using FTIR. Hourglass-shaped specimens were fabricated from both materials at each respective temperature and pulled apart to evaluate UTS after 48 h storage. Data were analyzed by ANOVA/Tukey’s test/Pearson’s correlation (p = 0.05). Neither adhesive/composite temperature nor their interaction had a significant effect on µSBS. No significant difference in µSBS between groups, except within 40 °C FBU. Predominant failure mode was a mixed type. No significant difference in DC% of FBU groups. RDC at 40 °C had significantly higher DC% than 25 °C. No significant difference in UTS of FBU and RDC groups. Application of both dual-polymerized adhesive and resin composite at 40 °C seemed to reduce µSBS. Raising the temperature to 40 °C improved DC% of resin composite, with no effect on adhesive. Pre-heating did not influence the UTS of both materials.
Background: Early childhood caries (ECC) is a common dental condition that could affect preschool children ‘s functional and emotional well-being worldwide. Therefore, this study aimed to evaluate the impact of ECC on preschool Egyptian children’s Oral Health Related Quality of Life (OHRQoL) and their parents. Materials and methods: This observational cross-sectional study included 260 preschool children aged 3 to 5 years who attended the Pediatric Outpatient Clinic at Ain Shams University. A resident dentist performed clinical examinations to measure the dmft index (decayed, missing, and filled teeth) using dental examination tools following the World Health Organization (WHO) criteria for diagnosing dental caries. Caries-free children were also included to enable direct comparison and estimate the impact of ECC severity on quality of life. The Arabic version of the Early Childhood Oral Health Impact Scale (A-ECOHIS) was used in this study to evaluate their OHRQoL. Data from the questionnaire were tabulated, summarized, and statistically analysed using Shapiro–Wilk, Mann–Whitney U and, the Kruskal–Wallis tests. Correlations assessments were made using Spearman’s rank correlation. Results: Out of 260 children who participated in the study, 75.8% had ECC, of whom 31% had ECC and 69% had severe ECC (S-ECC). The mean ECOHIS score was 19.52 ± 12.46. Children with S-ECC had a significantly higher mean ECOHIS score (25.87 ± 10.05) than children without caries (4.94 ± 6.08) and those with ECC (20.35 ± 8.96) ( p < 0.0001). Regression analysis verified that worse OHRQoL was significantly associated with the presence of ECC and rising dmft scores. Higher ECOHIS scores were also associated with maternal employment and parental age < 35 years. Conclusions: Lower OHRQoL was significantly associated with the high prevalence of ECC and severe ECC (S-ECC), especially in domains related to pain, eating difficulties, and psychological discomfort. Higher dmft scores, the presence of ECC, younger parental age, and employment were also associated with worse OHRQoL scores. These results emphasize the importance of early preventive dental care, particularly for preschool children in resource-limited settings.
Purpose: To investigate the influence of smoking and finishing and polishing protocol on color stability and surface roughness of resin composite. Materials and methods: Seventy-two discs fabricated from supra-nanofilled composite were divided to 6 groups according to: Tobacco Product (Conventional Cigarette/CS and Heated Tobacco/HTP); and Finishing and Polishing Protocol (Control/C, Multi-step finishing system/FS, and Medium-grit abrasive bur + two-step polishing system/PS). After finishing and polishing, specimens were exposed to a total of 600 cigarettes, divided into 20 each day, simulating 30 days of smoking. Color parameters were detected using a spectrophotometer. Surface roughness (Ra) was measured before and after smoking exposure using a surface roughness tester. Surface morphology was assessed under SEM. Data were analyzed using ANOVA/Tukey’s and student t-test. Results: For CS, ∆E values of C group was significantly higher than both finishing/polishing groups, which were statistically similar. For HTP, no significant difference in ∆E values between all groups. ∆E values of CS were significantly higher than HTP in all groups. For CS, C group showed significantly higher change in Ra than FS group; whilst no significant difference in Ra change values of PS and those of C and FS groups. For HTP, no significant difference in Ra change between all groups. Within C group, Ra change of both smoking groups was statistically similar. Within FS and PS groups, change in Ra of HTP was significantly higher than CS. Conclusion: Conventional cigarette smoking resulted in pronounced color change in the supra-nanofilled composite. While heated tobacco product produced an increased surface roughness. Both multi-step finishing system and two-step polishing system displayed comparable color change and surface roughness in supra-nanofilled composite.
The aim of this study was to evaluate the effect of surface treatment and storage time on immediate repair bond durability of methacrylate- and ormocer-based bulk fill composites. In total, 265 discs were divided into 32 groups (n = 8/group) according to: (1) Material: X-tra fil and Admira Fusion X-tra; (2) Surface treatment: oxygen inhibition; matrix; Futurabond M+; Silane/Futurabond M+; Admira Bond; Silane/Admira Bond; ceramic repair system; and Silane/Cimara bond; and (3) Storage time: 24 h and 6 months. Each disc received three micro-cylinders from the same material. Specimens were subjected to micro-shear bond strength testing either at 24 h or 6 months. Data were analyzed using ANOVA/Tukey’s test/Student t-test (p = 0.05). All experimental factors had significant effect on bond strength (p < 0.0001). Drop in bond strength was noticed in both materials after six months (p < 0.05), except for Admira Fusion X-tra treated with silane/cimara adhesive (p = 0.860). Both materials showed insignificant values with Admira bond either at 24 h or 6 months (p = 0.275 and p = 0.060, respectively). For other treatments, X-tra fil showed significantly higher values at 24 h and 6 months (p < 0.05). Ceramic repair system can be used to immediately repair both methacrylate- and ormocer-based composites.
The aim of this study was to investigate influence of curing mode of universal adhesives and dentin sealing approach on microtensile bond strength (MTBS) of CAD/CAM composite to dentin. Occlusal surfaces of 36 human molars were ground to expose flat dentin and randomly assigned to 6 groups according to: (1) Adhesive curing mode [light-cured/LC (One coat 7 Universal, COLTENE); dual-cure/DC (One coat 7 Universal/Dual-cure Activator, COLTENE); and self-cure/SC (Palfique Universal Bond, Tokuyama); and (2) Dentin sealing approach (delayed sealing/DDS and immediate sealing/IDS). Following 1-week provisionalization, CAD/CAM composite blocks (Brilliant Crios, COLTENE), 4 mm 2 , were cemented over conditioned dentin surfaces. After 24 h, bonded assemblies were thermo-cycled for 5000 cycles. Specimens were tested for MTBS. Failure mode was analyzed under stereomicroscope. Data were statistically analyzed using ANOVA. DDS showed significantly higher MTBS values than IDS when using LC and DC adhesives. While, IDS produced significantly higher MTBS values than DDS when using SC adhesive. Predominant failure mode was adhesive in all groups, except for SC adhesive in IDS group, mixed failure was the predominant mode. Light- and dual-cured universal adhesives improved bond strength in delayed dentin sealing approach. Self-cure universal adhesive produced better bond strength when applied to immediately sealed dentin.