Background: The effect of 3D printing technology and build angle on the marginal fit of printed crowns is unclear. The objective of this research was to use digital light processing (DLP) and stereo-lithography (SLA)-based 3D printing to construct single restorations with varied build angles and to analyze the crowns′ marginal fit. Methods: A prepared resin first molar was scanned utilizing an optical scanner. Three build orientations were used to construct the specimens: 0, 45, and 90º. DLP and SLA technology were used to produce the casting patterns. A digital microscope was used to measure the marginal gaps. The effect of build orientation was statistically analyzed by using Two-way ANOVA followed by pair-wise Tukey test. Results: Two-way ANOVA revealed a significant effect of printer technology and build angle on the marginal discrepancy of 3D printed crowns (p < 0.001). One-way ANOVA revealed that SLA printers (55.6 [± 13.59]) showed significantly better mean [± SD] marginal discrepancy in µm than DLP printers (72 [± 13.67]) (p < 0.001). Regarding build angle, one-way ANOVA revealed significant differences between the different angles. Tukeys post-hoc test revealed that 0° (48.5 [± 9.04]) had the significantly smallest marginal discrepancy followed by 45° (62.5 [± 8.05]) then 90° (80.5 [± 8.99]) (p < 0.001). Conclusion: The build orientation affects the marginal discrepancy of single crowns manufactured utilizing DLP and SLA.
This study evaluated the effect of surface treatment of zirconia in pre-sintered and post-sintered stages on its surface roughness, phase transformation, and biaxial flexural strength (BFS). Zirconia ceramic discs (n=40) having a final dimensions of 12mm diameter and 1.2mm thickness were milled then divided into three main groups according to the type of surface treatment performed (Group 1 (n=16); air-abrasion using Al2O3 particles, Group 2 (n=16); silica coating using Rocatec soft, and Group 3 (n=8); a control group receiving no surface treatment). Groups 1 and 2 were divided into two subgroups each according to the stage in which the surface treatment was performed (Subgroup A; surface treatment performed in the pre-sintered stage and subgroup B; surface treatment performed in the post-sintered stage). Surface roughness, phase transformation, and biaxial flexural strength (BFS) were later assessed. Data was then analyzed using two-way ANOVA and Tukey post-hoc tests at a significance level of p≤0.05. Subgroups treated in the pre-sintered stage showed higher mean Ra in μm (1.81±0.36) when compared to the subgroups treated in the post-sintered (0.68±0.07) stage and the control group (0.51±0.10) (p≤0.05). The pre-sintered treated group and the control showed no monoclinic phase while the post-sintered group showed significantly higher portions of monoclinic phase. Regarding BFS the post-sintered treated group had statistically significant higher values in MPa (1228±81) when compared to the pre-sintered treated group (940±101) and the control (1019±82) (p≤0.05). Air abrasion in the pre-sintered stage might be a promising surface treatment method to produce promising surface roughness values of zirconia without subjecting it to early degradation.
10 February 2022 in Journal of Esthetic and Restorative Dentistry