Coarse-grain heat-affected zone (CGHAZ) properties of steel deteriorate when it is welded using high heat input, which always restricts the promotion and use of high heat input welding steel. TiN particles significantly inhibit the growth of austenite and improve the microstructure and properties of high heat input welding steel. Effects of different Ti/N ratios on the CGHAZ microstructure and properties of high heat input welding steel were studied using welding thermal simulations and in situ observations. Results showed that a higher Ti/N ratio led to the abnormal growth of austenite grains and promoted the nucleation and growth of lath ferrite, which made the microstructure of the CGHAZ heterogeneous. In contrast, austenite grains were more uniform at a lower Ti/N ratio. Thus, the microstructure was refined, the brittle structure was reduced, and the properties of the CGHAZ were improved. In addition, when Ti/N = 5.85, the impact absorption energy of the CGHAZ obviously fluctuated. However, when Ti/N = 2.82, the impact absorption energy of the CGHAZ was higher and more stable. These results provided a new idea for the development of high heat input welding steel based on TiN theory.
Ultra-thick offshore steel, known for its high strength, high toughness, and corrosion resistance, is commonly used in marine platforms and ship components. However, when offshore steel is in service for an extended period under conditions of high pressure, extreme cold, and high-frequency impact loads, the weld joints are prone to fatigue failure or even fractures. Addressing these issues, this study designed a narrow-gap laser wire filling welding process and successfully welded a 100-mm new type of ultra-thick offshore steel. Using finite element simulation, EBSD testing, SEM analysis, and impact experiments, this study investigates the weld’s microstructure, impact toughness, and fracture mechanisms. The research found that at −80 °C, the welded joint exhibited good impact toughness (>80 J), with the impact absorption energy on the surface of the weld being 217.7 J, similar to that of the base material (225.3 J), and the fracture mechanism was primarily a ductile fracture. The impact absorption energy in the core of the weld was 103.7 J, with the fracture mechanism mainly being a brittle fracture. The EBSD results indicated that due to the influence of the welding thermal cycle and the cooling effect of the narrow-gap process, the grains gradually coarsened from the surface of the welded plate to the core of the weld, which was the main reason for the decreased impact toughness at the joint core. This study demonstrates the feasibility of using narrow-gap laser wire filling welding for 100-mm new type ultra-thick offshore steel and provides a new approach for the joining of ultra-thick steel plates.