Elastomeric materials are often used as components that undergo cyclic loading during application, such as tires, seals, and hoses. For this reason, the long-term performance, or more precisely the crack growth behavior, is of great importance. Even though several studies investigated the fatigue behavior of rubber materials during the last 80 years, this topic is still widely under discussion and remains of great interest among scientists. Mars and Fatemi reviewed the developments of the field in the beginning of 2000, however, this paper considers the overall development including new findings to serve as a guide for further investigations in the field of fatigue of elastomers. For this purpose, the usual measurement methods and their evaluation, as well as the most important factors influencing the fatigue behavior, like the formulation of the rubber compound or the application and testing conditions, are explained in detail. Furthermore, an outlook is given on parameters that still need to be scientifically investigated, such as the influence of filler orientations or the selected manufacturing method, in order to fully understand fatigue crack growth.
Predicting the curing behaviour of industrially employed elastomeric compounds under typical processing conditions in a reliable and scientifically driven way is important for rubber processing simulation routines, such as injection moulding. Herein, a rubber process analyser was employed to study the crosslinking kinetics of solid silicone rubber based on the concentration of dicumylperoxide. A model was proposed to describe the optimal cure time variation with peroxide concentration and temperature, based on the analysis of processing parameters applying kinetic and thermodynamic judgments. Additionally, the conversion rate was described with the aid of a phenomenological model, and the effect of dicumylperoxide concentration on the final crosslink state was investigated using kinetic and thermodynamic explanations. Optimal curing time was affected both by temperature and dicumylperoxide concentration. However, the effects were less pronounced for high temperatures (>170 C) and high concentrations (>0.70 phr). A limit on the crosslink state was detected, meaning that the dicumylperoxide capacity to crosslink the silicone network is restricted by the curing mechanism. Curing restrictions were presumed to be primarily thermodynamic, based on the proton abstraction mechanism that drives the crosslinking reaction. In addition to providing more realistic crosslinking models for rubber injection moulding simulation routines, the results of this study may also explain the chemical behaviour of organic peroxides widely used for silicone crosslinking.
Application of elastomers in general demands the conversion of their soluble networks into crosslinked structures. This abrupt change causes several modifications, both in the atomic/molecular level and at the macro‐scale. In this study, solid silicone rubber (high molecular weight poly(dimethylsiloxane)), was crosslinked with dicumylperoxide (DCP), a widely used crosslinking agent by the rubber industry. The changes caused by different DCP concentrations were investigated, aiming to bring attention to the molecular transformations, usually neglected when processing‐oriented studies are conducted. DCP concentration showed a limited contribution to the network's molecular dynamics, which was found to be mainly dominated by entanglements. The dominance of entanglements over other molecular constraints, like crosslink points, justifies the threshold and counter‐intuitive behavior of tensile and hardness properties. However, differences were found in the crystallization ability after crosslinking, when the more crosslink points were introduced, the lower the crystallinity was and the less stable the PDMS crystallites were. In addition to providing a deeper understanding of an industrially applied rubber system n terms of the effective concentration of DCP, and the reasoning behind such concentration, the findings of this study add to the state‐of‐the‐art comprehension of elastomeric networks, and how they behave on a molecular level.
Computational fluid dynamics (CFD) simulation is an important tool as it enables engineers to study different design options without a time-consuming experimental workload. However, the prediction accuracy of any CFD simulation depends upon the set boundary conditions and upon the applied rheological constitutive equation. In the present study the viscoelastic nature of an unfilled gum acrylonitrile butadiene rubber (NBR) is considered by applying the integral and time-dependent Kaye–Bernstein–Kearsley–Zapas (K-BKZ) rheological model. First, exhaustive testing is carried out in the linear viscoelastic (LVE) and non-LVE deformation range including small amplitude oscillatory shear (SAOS) as well as high pressure capillary rheometer (HPCR) tests. Next, three abrupt capillary dies and one tapered orifice die are modeled in Ansys POLYFLOW. The pressure prediction accuracy of the K-BKZ/Wagner model was found to be excellent and insensitive to the applied normal force in SAOS testing as well as to the relation of first and second normal stress differences, provided that damping parameters are fitted to steady-state rheological data. Moreover, the crucial importance of viscoelastic modeling is proven for rubber materials, as two generalized Newtonian fluid (GNF) flow models severely underestimate measured pressure data, especially in contraction flow-dominated geometries.
Injection molding of rubber compounds is an easily conducted yet sophisticated method for rubber processing. Simulation software is used to examine the optimal process conditions, identify failure scenarios, and save resources. Due to the complexity of the entire process, various aspects have to be considered in the numerical approach. This contribution focused on a comparison of process simulations with various definitions of the material’s inlet temperature, ranging from a stepwise increase, but constant temperature, to an exact axial mass temperature profile prior to injection. The latter was obtained with a specially designed, unique test stand consisting of a plasticizing cylinder equipped with pressure sensors, a throttle valve for pressure adjustments, and a measurement bar with thermocouples for the determination of the actual state of the mass temperature. For the verification of the theoretical calculations, practical experiments were conducted on a rubber injection molding machine equipped with the mold used in the simulation. The moldings, obtained at different vulcanization time, were characterized mechanically and the results were normalized to a relative degree of cure in order to enable comparison of the real process and the simulation. Considering the actual state of the mass temperature, the simulation showed an excellent correlation of the measured and calculated mass temperatures in the cold runner. Additionally, the relative degree of cure was closer to reality when the mass temperature profile after dosing was applied in the simulation.