The scientific community has shown a growing interest in relating to the ferroelectric materials and it has made an effort to develop them. Among these several ferroelectric materials, we proposed to investigated Pb(ZrTi)O3 doped with distinct Er+3 concentrations. Our aim was to investigate how the erbium affects the PZT electrical properties. To determine the ideal sintering temperature of our ceramic samples, the dilatometry tests were performed. These results have showed that the erbium caused a change in sample densities (91.9% < ρ < 99.0%) as compared to undoped PZT sample. Furthermore, the X-ray diffraction results indicated that all samples are monophasic and peaks are indexed to tetragonal crystalline structure. According to these also results, there was an increment of the parameter a and a reduction of parameter c as compared to undoped PZT sample. On the other hand, the average grain size have decreased with the increment of erbium content. The electrical characterization of ours ceramics showed a peculiar ferrelectric-paraeletric phase transition around 390 ºC. Finally, the ferroelectric hysteresis measurements for doped samples in site A have revealed that remnant polarization and coercive field values depend on content. Whereas, doped samples in site B, the corresponding values are similar.
1 January 2022 in Journal of Physics and Chemistry of Solids
The reduction kinetics of hematite (Fe2O3) powders was studied using nonequilibrium hydrogen plasma as reducing agent. Reduction experiments were performed in a DC pulsed plasma reactor, hydrogen flow-rate of 300 cm3/min, at pressure of 400 Pa, reduction times in range 30-120 minutes and in temperatures range 320-380 °C. Fe2O3 powders after reduction experiments were characterized by X-ray diffraction, weight loss of oxygen (gravimetric analyses), optic microscope and scanning electron microscope. The results showing that the reduction temperature of 380 °C after 120 min allows obtaining α-iron with a reduction fraction of about 0.93. The powder particles are transformed into two steps: Fe2O3→Fe3O4→Fe-α. The activation energy experimentally established for the reduction of Fe2O3 was about 98.4 kJ/mol.
High chromium cast irons (HCCIs) are widely applied in the mining industry as components of equipment for iron ore transportation, in which their surfaces are subjected to abrasive and erosive wear. The present work evaluated the erosion-abrasion behavior of a HCCI possessing different amounts of austenite and martensite, using a laboratory impeller-tumbler wear test apparatus and iron ore pellets as abrasive material. The results showed that the wear dominant mechanism on the worn surface of the as-cast material depends upon the material microstructure. For HCCI destabilized at 930 and 990 °C, the matrix has high martensite/austenite ratio and finely dispersed secondary carbides, offering high abrasion-erosion wear resistance. The absence of fractured eutectic carbides indicates that such matrix has hardness and load bearing capacity, enough for mitigating a significant plastic deformation during the impact pellets. For HCCI destabilized at 1050 °C, the matrix has a low martensite/austenite ratio and coalesced secondary carbides, leading to high wear rates during erosion-abrasion tests.
The reduction of cobalt oxide (Co3O4) powders was studied using hydrogen plasma (HP) and hydrogen gas at low temperatures. The reduction experiments were performed in a pulsed plasma reactor at 540 V, 532 Pa, under atmospheres of 100% hydrogen at a flow rate of 300 cm3/min, with varying times up to 60 min, and temperature range of 523–653 K. The results showed that the reduction of Co3O4 powders occurs in two steps: Co3O4 → CoO → Co, when using either HP or hydrogen gas. At lower temperatures, hydrogen plasma provided a significant increase in reduction kinetics compared to gas, since atomic hydrogen is a more powerful reductant than molecular hydrogen due to the increase in the density of crystalline defects provoked by the impact of ions incidents contained in plasma.The values for the activation energy were determined to be 35.4 kJ/mol for plasma and 90.8 kJ/mol for gas, and the kinetic equation that best fits to both experimental data was [1 – (1 – α)1/3 ]2 = k.t.