Mohamed Yacine Debili

Prof. Mohamed Yacine Debili


Research Focus & Metrics

Academic Career Length

39Years (1988-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 January 2004 in Physica Scripta
Verified
Journal Article
Closed access
MDM Draissia
M Draissia
HBH Boudemagh
H Boudemagh
MDMohamed Yacine Debili
Mohamed Yacine Debili

1 September 2005 in Open Physics
Verified
Journal Article
Open access
PDF file
MDMohamed Draissia
Mohamed Draissia
MDMohamed Yacine Debili
Mohamed Yacine Debili
Solid-solution formation in binary aluminium-based alloys is due essentially to the combined effects of the size and valence of solvent and solute atoms, as expected by the four Hume-Rothery rules. The lattice parameter of aluminium in the solid solution of the sputtered Al−Fe films is [Al-a (Å)=4.052−6.6×10−3Y]. The increasing and decreasing evolution of the lattice parameter of copper [Cu-a (Å)=3.612+1.8×10−3Z] and aluminium [Al-a (Å)=4.048−1.6×10−3X] in the sputtered Al-1.8 to 92.5 at. % Cu films is a result of the difference in size between the aluminium and copper atoms. The low solubility of copper in aluminium (<1.8 at % Cu) is due to the valences of solvent and solute atoms in contrast with other sputtered films prepared under similar conditions, such as Al−Mg (20 at. % Mg), Al−Ti (27 at. % Ti), Al−Cr (5at. % Cr) and Al−Fe (5.5 at. % Fe) where the solubility is due to the difference in size.

1 September 2004 in Journal of Crystal Growth
Verified
Journal Article
Closed access
MDM. Draissia
M. Draissia
MDMohamed Yacine Debili
Mohamed Yacine Debili

17 February 2009 in The European Physical Journal Applied Physics
Verified
Journal Article
Closed access
PDF file
NBN. Boukhris
N. Boukhris
SLS. Lallouche
S. Lallouche
MDMohamed Yacine Debili
Mohamed Yacine Debili
MDM. Draissia
M. Draissia
The materials under consideration are binary aluminium-copper alloys (10 at% to 90.3 at%Cu) produced by HF melting and RF magnetron sputtering. The resulting micro structures have been observed by standard metallographic techniques, X-ray powder diffraction, scanning electron microscopy and transmission electron microscopy. Vickers microhardness of bulk Al–Cu alloys reaches a maximum of 1800 MPa at 70.16 at%Cu. An unexpected metastable phase has been observed within aluminium grain in Al-37 at%Cu. The mechanical properties of a family of homogeneous AlCu x (0 < x < 0.92) thin films made by radiofrequency (13.56 MHz) cathodic magnetron sputtering from composite Al–Cu targets have been investigated. The as-deposited microstructures for all film compositions consisted of a mixture of the two expected face-centred-cubic (fcc) Al solid solution and tetragonal θ (Al2Cu) phases. The microhardness regularly increases and the grain size decreases both with copper concentration. This phenomenon of significant mechanical strengthening of aluminium by means of copper is essentially due to a combination between solid solution effects and grain size refinement. This paper reports some structural features of different Al–Cu alloys prepared by HF melting and RF magnetron on glass substrate sputtering.

1 December 1998 in Revue de Métallurgie
Verified
Journal Article
Closed access
PDF file
MDMohamed Yacine Debili
Mohamed Yacine Debili
TLTran Huu Loï
Tran Huu Loï
CFC. Frantz
C. Frantz
Metallurgical Research & Technology, an international journal for steel and other metals: from making to using

1 August 2005 in Philosophical Magazine Letters
Verified
Journal Article
Closed access
MDM. Draissia
M. Draissia
MDMohamed Yacine Debili
Mohamed Yacine Debili
The microstructures of Al–1.8 to 92.5 at.% Cu thin films prepared by radiofrequency (13.56 MHz) cathodic magnetron sputtering have been investigated by X-ray diffraction (XRD) and transmission electronic microscopy (TEM). A phase separation occurs in films of nominal Al–66.64 at.% Cu composition, consisting of a fcc Al solid solution phase, a fcc Cu solid solution phase and an unexpected sc Cu3Al ordered phase with a Cu3Au structure and a lattice parameter of about 0.36 nm.