Lightweight electromagnetic interference shielding cellulose foam/carbon fiber composites were prepared by blending cellulose foam solution with carbon fibers and then freeze drying. Two kinds of carbon fiber (diameter of 7 μm) with different lengths were used, short carbon fibers (SCF, L/D = 100) and long carbon fibers (LCF, L/D = 300). It was observed that SCFs and LCFs built efficient network structures during the foaming process. Furthermore, the foaming process significantly increased the specific electromagnetic interference shielding effectiveness from 10 to 60 dB. In addition, cellulose/carbon fiber composite foams possessed good mechanical properties and low thermal conductivity of 0.021–0.046 W/(m·K).
The nanometer zinc complex, formed in chloride-urea ionic liquid (IL), was studied with the objective of enhancing the mildew resistance of bamboo. The nano-Zinc complex layer was coated on the bamboo surface by a simple and mild heating process. The SEM analysis revealed that the morphology of the nanometer Zinc complex layer on the bamboo surface varied with the reaction time of bamboo in zinc chloride (ZnCl2)/urea ionic liquid. The result of EDS and FTIR analysis showed that zinc and chlorine were successfully coated on the surface of bamboo. In this study, it was found that the optimum condition was 2 h of reaction with 1:2 molar ratio of zinc chloride to urea, where the nano-Zinc complex layer on the bamboo surface was the most uniform and dense to present the bamboo with the strongest mildew resistance. The infection value of Trichoderma viride, Aspergillus niger V. Tiegh, and Penicillium citrinum Thom after 28 day was 0.
Practical application of wood remains a great challenge because of its highly hydrophilic property. In this work, highly hydrophobic wood was produced using an environment-friendly and two-component package method. Poly(methylhydrogen)siloxane (PMHS) and inhibitor played the key role in the hydrophobicity of wood and the assembly process. The two-component package mechanism was discussed in detail. As a result, the water contact angles of the modified wood surface for the radial and cross sections were 139.5° and 152.9°, respectively, which provided the resultant wood high hydrophobicity and dimensional stability. The two-component package method afforded the wood good anti-fouling property and UV-resistance. In addition, the two-component package method could also be applied in functionalization of filter paper for oil/water separation.