Deformation mechanisms in extruded Mg-Y-Zn alloys with different volume fractions of the long-period stacking ordered (LPSO) structure have been investigated during cyclic loading, i.e., compression followed by unloading and reverse tensile loading. Electron backscattered diffraction (EBSD) and in situ neutron diffraction (ND) techniques are used to determine strain path dependence of the deformation mechanisms. The twinning-detwinning mechanism operated in the α-Mg phase is of key importance for the subsequent hardening behavior of alloys with complex microstructures, consisting of α-Mg and LPSO phases. Besides the detailed analysis of the lattice strain development as a function of the applied stress, the dislocation density evolution in particular alloys is determined.
Precipitation of γ’ phase in nickel-base superalloy IN792-5A was studied using in-situ Small Angle Neutron Scattering (SANS). It was found that additional precipitates are formed after reheating above 600 °C when the material is previously fast cooled (100 K/min) from 900 °C. The size distribution and volume fraction of the additional γ’ precipitates as well as of the already present medium-size precipitates in dependence on temperature were evaluated. The small precipitates can influence mechanical properties of the alloy, which exhibits an anomaly in the temperature dependence of the yield stress. Volume fraction of all precipitate populations above 900 °C was estimated as well.
Twin roll casting (TRC), with a relatively fast solidification rate, is an excellent production method with promising potential for producing wrought semi or final Mg alloy products that can often suffer from poor formability. We investigate in this study the effect of the TRC method and the subsequent heat treatment on the microstructure and deformation mechanisms in Mg-Zn-Zr-Nd alloy deformed at room temperature using the in-situ neutron diffraction and acoustic emission techniques and ex-situ texture measurement and microscopy, respectively. Although a higher work hardening is observed in the rolling direction due to the more intensive <a>-type dislocation activity, the difference in the mechanical properties of the specimens deformed in the RD and TD directions is small in the as-rolled condition. An additional heat treatment results in recrystallization and significant anisotropy in the deformation. Due to the easier activation of the extension twinning in the TD given by texture, the yield stress in the TD is approximately 40% lower than that in the RD.
23 November 2013 in Metallurgical and Materials Transactions A
Boron largely increases the ductility of polycrystalline high-temperature Co–Re–Cr alloys. Therefore, the effect of boron addition on the alloy structural characteristics is of large importance for the stability of the alloy at operational temperatures. Along with the Co-solid solution matrix phase transformation from hcp to fcc structure, additional structural effects were observed in situ at very high temperatures (up to 1500 °C) using neutron diffraction (ND) in boron-containing Co–17Re–23Cr alloys. Increasing boron content up to 1000 wt. ppm lowers the temperature at which sublimation of Co and Cr from the matrix occurs. As a result, the composition of the matrix in the surface region is changed leading to the formation of a second and a third matrix hcp phases at high temperatures. The consideration on the lattice parameter dependence on composition was used to identify the new phases appearing at high temperatures. Energy-dispersive spectroscopy and ND results were used to estimate the amount of Co and Cr which sublimated from the surface region of the high-boron sample. In the sense of alloy development, the sublimation of Co and Cr is not critical as the temperature range where it is observed (≥1430 °C) is significantly above the foreseen operation temperature of the alloys (1200 °C).
21 February 2020 in Journal of Applied Crystallography