SUMMARY: Objectives: To evaluate the effects of surface treatment, specimen thickness, and aging on the biaxial flexural strength (BFS) of two types of yttria-stabilized, tetragonal zirconia polycrystal (Y-TZP) ceramics.Methods and Materials: Disc-shaped specimens, 0.4 and 1.3 mm thick, made from hot isostatic pressed (Denzir) and non–hot isostatic pressed (ZirPlus) Y-TZP, were sandblasted, heat treated, and autoclaved. The surface topography was assessed in accordance with European Standard 623-624:2004 and the BFS tests in accordance with International Organization for Standardization Standard 6872:2008. For statistical analyses, one-way Shapiro-Wilk test, analysis of variance (post hoc: least significant differences), Mann-Whitney U-test, and Pearson correlation tests (p1.3-mm ZirPlus (p1.3-mm Denzir (p<0.001). Sandblasting with 0.2 MPa reduced the BFS of the ZirPlus and Denzir discs (p<0.01), whereas sandblasting with 0.6 MPa increased the BFS of the 0.4-mm Denzir (p<0.001) and reduced the BFS of the 0.4-mm ZirPlus (p<0.05). Heat treatment significantly reduced the BFS of all the groups except for the 0.6 MPa sandblasted 0.4-mm ZirPlus. Autoclaving reduced the BFS of the as-delivered ZirPlus and Denzir specimens (p0.05) on the BFS. The 0.6 MPa sandblasted, heat-treated, and autoclaved 0.4-mm Denzir exhibited higher BFS than the 0.6 MPa sandblasted, heat-treated, and autoclaved 0.4-mm ZirPlus (p<0.05).Conclusions: Thickness and surface treatment of Y-TZP–based ceramics should be considered since those factors could influence the BFS of the material.
1 October 2015 in Journal of the Mechanical Behavior of Biomedical Materials
Using a newly developed three-dimensional (3D) numerical modeling code, an analysis was performed of the fracture behavior in a three-unit ceramic-based fixed partial denture (FPD) framework subjected to oblique loading. All the materials in the study were treated heterogeneously; Weibull׳s distribution law was applied to the description of the heterogeneity. The Mohr-Coulomb failure criterion with tensile strength cut-off was utilized in judging whether the material was in an elastic or failed state. The simulated loading area was placed either on the buccal or the lingual cusp of a premolar-shaped pontic with the loading direction at 30°, 45°, 60°, 75° or 90° angles to the occlusal surface. The stress distribution, fracture initiation and propagation in the framework during the loading and fracture process were analyzed. This numerical simulation allowed the cause of the framework fracture to be identified as tensile stress failure. The decisive fracture was initiated in the gingival embrasure of the pontic, regardless of whether the buccal or lingual cusp of the pontic was loaded. The stress distribution and fracture propagation process of the framework could be followed step by step from beginning to end. The bearing capacity and the rigidity of the framework vary with the loading position and direction. The framework loaded with 90° towards the occlusal surface has the highest bearing capacity and the greatest rigidity. The framework loaded with 30° towards the occlusal surface has the least rigidity indicating that oblique loading has a major impact on the fracture of ceramic frameworks.