The pursuit of reliable energy devices sealing solutions stands as a paramount engineering challenge for ensuring energy safety and dependability. This review focuses on an examination of recent scientific publications, primarily within the last decade, with a central aim to grasp and apply critical concepts relevant to the efficient design and specification of brazements for ceramic–metal active-brazed assemblies, emphasizing the sealing of energy devices. The goal is to establish robust and enduring joints capable of withstanding water-vapor and hydrogen environments. The review commences with a concise recapitulation of the fundamental principles of active brazing, followed by an in-depth exploration of material selection, illustrated using water-vapor-resistant sensors as illustrative examples. Furthermore, the review presents practical solutions for the sealing of energy devices while also scrutinizing the factors that exert significant influence on the deterioration of these active-brazed connections. Ultimately, the review culminates in a comprehensive discussion of emerging trends and developments in active brazing techniques for energy-related applications.
Lower bainite can indeed grow below martensite start temperature ( MS ) in a commercial alloy. Ultrahigh-strength low-alloyed 42CrMo4 steels are austempered below MS . The preliminary martensite and lower bainite packets formed during austempering partition the prior austenite grains effectively. The obtained ultrafine-grained nanostructured microstructure enhances the mechanical properties of the alloys significantly. Morphology and overall microstructure are examined by reflection optical microscope and scanning electron microscopy. Substructures of lower bainite and virgin/tempered martensite are revealed by transmission electron microscopy. With increasing duration of austempering, a clear transition from cleavage to ductile rupture was observed by fractography. Effects of grain partitioning and the risk of embrittlement have been discussed concretely. The better understanding of the microstructure austempered below MS will feedback to the materials development activities both in conventional and new materials areas.
27 February 2024 in Journal of Materials Engineering and Performance
The development of reliable joining techniques for ceramics and metals is crucial for energy applications, such as fuel cells, nuclear reactors, and high-temperature sensors, most especially for the sealing of hydrothermal sensors to study multiphase flows. However, during one-step active laser brazing it is a serious problem that a high thermal stress concentration can occur at the joint interfaces or on the ceramic side of the joint due to mismatches between the CTEs (coefficients of thermal expansion) and/or elastic constants. The uncontrolled thermal residual stress can lead to cracks and defects in the brazement. In the present work, an elastoplastic finite element method/numerical model was formulated to study the thermal residual stresses developed in the brazement between ceramics and austenitic stainless steel during cooling in active laser brazing. Calculations and comparison experiments were conducted to validate the simulated stress distribution in un-patterned ceramics. Stress analyses were conducted for planar and cylindrical specimen geometries (lab joints) relevant for miniaturized energy sensors. Laser interface patterning was employed to create micro-scale features on ceramic interfaces that reduce thermal stress concentrations. The optimization of the interface designing parameters including hatch size, structure width, pattern depth and metal/ceramic thickness ratio was performed using the Taguchi method with orthogonal arrays. The study suggests that laser interface structuring can modify thermal residual stresses in ceramic-to-metal brazements, thereby increasing the reliability of active brazing joints.