The fabrication of high-precision scaffolds with excellent biocompatibility for tissue engineering has become a research hotspot. Two-photon polymerization (TPP) can break the optical diffraction limit and is used to fabricate high-resolution three-dimensional (3D) microstructures. In this study, the biological properties, and machinability of photosensitive gelatin methacrylate (GelMA) hydrogel solutions are investigated, and the biocompatibility of 3D scaffolds using a photosensitive GelMA hydrogel solution fabricated by TPP is also evaluated. The biological properties of photosensitive GelMA hydrogel solutions are evaluated by analyzing their cytotoxicity, swelling ratio, and degradation ratio. The experimental results indicate that: (1) photosensitive GelMA hydrogel solutions with remarkable biological properties and processability are suitable for cell attachment. (2) a micro/nano 3D printed scaffold with good biocompatibility is fabricated using a laser scanning speed of 150 μm/s, laser power of 7.8 mW, layer distance of 150 nm and a photosensitive GelMA hydrogel solution with a concentration of 12% (w/v). Micro/nano additive manufacturing will have broad application prospects in the tissue engineering field.
Excellent biocompatibility and corrosion resistance of implants are essential for Ti6Al4V parts fabricated by selective laser melting (SLM) for biomedical applications. To achieve better corrosion resistance and biocompatibility of Ti6Al4V parts, the effects of SLM processing parameters on the corrosion resistance and the biocompatibility of Ti6Al4V parts are investigated by changing the scanning speeds and laser powers. The detailed influence mechanism of processing parameters on the properties of Ti6Al4V parts is studied from two aspects, including microstructure and defects. It is found that the corrosion resistance and biocompatibility of Ti6Al4V parts can be adjusted by changing the scanning speed and the laser power due to the constituent phase and the number and size of defect holes of Ti6Al4V parts. Compared with the laser power, the scanning speed has a stronger influence on the performance of the part, which can be used as “coarse tuning” based on the performance requirements. At the scanning speed of 1100 mm/s and the laser power of 280 W, Ti6Al4V parts with better corrosion resistance can be obtained. Ti6Al4V parts with better biocompatibility are fabricated at the scanning speed of 1200 mm/s and the laser power of 200 W.
In this study, a continuous fiber laser (1064 nm wavelength, 30 W/cm2) is used to irradiate multi-walled carbon nanotubes (MWCNTs) on different substrate surfaces. Effects of substrates on nano-welding of MWCNTs are investigated by scanning electron microscope (SEM). For MWCNTs on silica, after 3 s irradiation, nanoscale welding with good quality can be achieved due to breaking C–C bonds and formation of new graphene layers. While welding junctions can be formed until 10 s for the MWCNTs on silicon, the difference of irradiation time to achieve welding is attributed to the difference of thermal conductivity for silica and silicon. As the irradiation time is prolonged up to 12.5 s, most of the MWCNTs are welded to a silicon substrate, which leads to their frameworks of tube walls on the silicon surface. This is because the accumulation of absorbed energy makes the temperature rise. Then chemical reactions among silicon, carbon and nitrogen occur. New chemical bonds of Si–N and Si–C achieve the welding between the MWCNTs and silicon. Vibration modes of Si3N4 appear at peaks of 363 cm−1 and 663 cm−1. There are vibration modes of SiC at peaks of 618 cm−1, 779 cm−1 and 973 cm−1. The experimental observation proves chemical reactions and the formation of Si3N4 and SiC by laser irradiation.