Background: This study evaluated the effect of interim restorative materials (acrylic resin (AR), resin composite (RC) or polyetheretherketone (PEEK) for dental computer-aided design/computer-aided manufacturing (CAD/CAM)) on the stress distribution of a posterior three-unit fixed partial denture. Methods: The abutment teeth (first molar and first premolar) were modeled using the BioCAD protocol containing 1.5 mm of axial reduction and converging axial walls. A static structural analysis was performed in the computer-aided engineering software, and the Maximum Principal Stress criterion was used to analyze the prosthesis and the cement layers of both abutment teeth. The materials were considered isotropic, linearly elastic, homogeneous and with bonded contacts. An axial load (600 N) was applied to the occlusal surface of the second premolar. Results: Regardless of the restorative material, the region of the prosthetic connectors showed the highest tensile stress magnitude. The highest stress peak was observed with the use of RC (129 MPa) compared to PEEK and AR. For the cement layers, RC showed the lowest values in the occlusal region (7 MPa) and the highest values for the cervical margin (14 MPa) compared to PEEK (21 and 12 MPa) and AR (21 and 13 MPa). Conclusions: Different interim restorative materials for posterior fixed partial dentures present different biomechanical behavior. The use of resin composite can attenuate the stress magnitude on the cement layer, and the use of acrylic resin can attenuate the stress magnitude on the connector region.
1 January 2019 in Journal of Clinical and Experimental Dentistry
To evaluate the stress distribution in a maxillary central incisor with different post and cores made of six CAD/CAM materials with different elastic modulus in the absence of ferrule using the finite element analysis. A three-dimensional endodontically treated maxillary central incisor restored with an all-ceramic crown was modelled in Rhinoceros (5.0 SR8, McNeel). The geometries were analyzed in ANSYS 17.2 (ANSYS Inc.) considering isotropic, homogeneous, linearly elastic materials with perfectly bonded contacts. The elastic moduli (E) of the post-and-cores defined the groups to be compared: nanoceramic resin (E=12.8GPa); composite resin (E=16GPa); hybrid ceramic (E=34.7GPa); lithium disilicate (E=95GPa); titanium (Ti-Al6-V4) (E=112GPa); and Y-TZP material (E=209.3GPa). The set was constrained in the cortical bone and loaded (45°/100 N) on the incisor palatine face. Stress distribution was analyzed by Maximum Principal Stress criteria for the crown-core cement line, Post-and-core's cement line, Post-and-core system and Dentin. The stress distribution at the crown-core cement line (11.4 - 13.2 MPa) was inversely proportional to the increase of the elastic modulus of the post-core approaches, while it was direct proportional on the post-and-core (4.7 - 40 MPa) and cement line (4.1 - 6.2 MPa). Stress distribution on the dentin was similar for all groups (24.7 - 25.3). Post-and-core made by CAD/CAM seems to be an efficient treatment alternative, since it is a conservative approach, promotes better aesthetic quality and it allows the control of the cement line thickness. Key words:Endodontically treated teeth, Post-and-core technique, Ceramic crown, Finite element analysis, Biomimetics.
This study evaluated the effect of the combination of three different onlay preparation designs and two restorative materials on the stress distribution, using 3D-finite element analysis. Six models of first lower molars were created according to three preparation designs: non-retentive (nRET), traditional with occlusal isthmus reduction (IST), and traditional without occlusal isthmus reduction (wIST); and according to two restorative materials: lithium-disilicate (LD) and nanoceramic resin (NR). A 600 N axial load was applied at the central fossa. All solids were considered isotropic, homogeneous, and linearly elastic. A static linear analysis was performed, and the Maximum Principal Stress (MPS) criteria were used to evaluate the results and compare the stress in MPa on the restoration, cement layer, and tooth structure (enamel and dentin). A novel statistical approach was used for quantitative analysis of the finite element analysis results. On restoration and cement layer, nRET showed a more homogeneous stress distribution, while the highest stress peaks were calculated for LD onlays (restoration: 69–110; cement layer: 10.2–13.3). On the tooth structure, the material had more influence, with better results for LD (27–38). It can be concluded that nRET design showed the best mechanical behavior compared to IST and wIST, with LD being more advantageous for tooth structure and NR for the restoration and cement layer.
This study evaluated the stress distribution in five different class II cavities of premolar models restored with conventional or bulk-fill flowable composite by means of finite element analysis (FEA) under shrinkage and occlusal loading. An upper validated premolar model was imported in the software, and five class II cavities with different occlusal extensions and dimensions were prepared: horizontal cavity on the mesial surface (horizontal slot), mesio-occlusal cavity, mesial cavity (vertical slot), tunnel type cavity and direct access cavity. The models were restored with conventional or bulk-fill flowable resin composite. The tested materials were considered as homogeneous, linear, and isotropic. The Maximum Principal Stress criteria was chosen to evaluate the tensile stress results. The lowest shrinkage stress value was observed in the direct access cavity restored with bulk-fill flowable resin composite (36.12 MPa). The same cavity, restored with conventional composite showed a score of 36.14 MPa. The horizontal slot cavity with bulk-fill flowable showed a score of 46.71 MPa. The mesio-occlusal cavity with bulk-fill flowable had a score of 53.10 MPa, while with conventional composite this was 55.35 MPa. Higher shrinkage stress was found in the vertical slot cavity with conventional resin 56.14 MPa, followed by the same cavity with bulk-fill flowable 56.08 MPa. Results indicated that the use of bulk-fill flowable composite resin more significantly decreased the polymerization shrinkage stress magnitude. The larger the cavity and the volume of material necessary to restore the tooth, the greater the residual stress on enamel and dentin tissue.
1 September 2021 in Journal of the Mechanical Behavior of Biomedical Materials
Background: Carious lesions and dental fractures cause weakening in the dental structure. In these situations, endodontic treatment and prosthetic rehabilitation using an intraradicular post are indicated. However, the postspace preparation of the root canal further weakens the dental remnant, especially if there is no ferrule present. This study aimed to evaluate the stress distribution in endodontically treated upper premolars treated with different rehabilitation approaches. Materials and Methods: An endodontically treated first upper premolar was modeled for finite element analysis. Three different approaches were carried out on this model: rehabilitation with fiberglass post (FCP), endocrown (ECW), or buildup. The models were exported in STEP format to the analysis software (ANSYS 17.2, ANSYS Inc., Houston, TX, USA). The solids were considered isotropic, homogeneous, and linearly elastic. A mechanical, structural static analysis was used as the criterion of maximum principal stress to show regions under tensile stress to evaluate the stress distribution in the restoration, cementation line, and root. A load of 400 N (90°) was applied to the lingual triangular ridge. The values of maximum principal stress in MPa were evaluated through colorimetric graphs. Results: Similar stress concentration was observed for all groups. However, the ECW group presented higher values in the restoration/cement interface and root dentin. Conclusions: All the treatment modalities had favorable mechanical behavior to support the masticatory loads; nevertheless, the ECW group presented a higher risk of detachment failure.