Local droplet etching (LDE) utilizes metal droplets during molecular beam epitaxy for the self-assembled drilling of nanoholes into III/V semiconductor surfaces. An essential process during LDE is the removal of the deposited droplet material from its initial position during post-growth annealing. This paper studies the droplet material removal experimentally and discusses the results in terms of a simple model. The first set of experiments demonstrates that the droplet material is removed by detachment of atoms and spreading over the substrate surface. Further experiments establish that droplet etching requires a small arsenic background pressure to inhibit re-attachment of the detached atoms. Surfaces processed under completely minimized As pressure show no hole formation but instead a conservation of the initial droplets. Under consideration of these results, a simple kinetic scaling model of the etching process is proposed that quantitatively reproduces experimental data on the hole depth as a function of the process temperature and deposited amount of droplet material. Furthermore, the depth dependence of the hole side-facet angle is analyzed.
The electron escape from self-assembled InAs quantum dots embedded in GaAs-Schottky diodes is probed with time-resolved capacitance measurements. We present the tunneling-transient spectroscopy technique to derive information on the barrier potential and the quantum dot level structure from the electric-field dependence of the capacitance transients. The data reveal that emission from - and -like quantum dot states can clearly be resolved. The barrier potential derived with this method in a simple triangular well model is in good agreement with values derived from measurements of the thermionic emission, if the emission from the -type dot level is analyzed. The emission from dots occupied with more than one electron is discussed within a simple one-dimensional tunneling model. It reveals that the triangular well model underestimates the well potential by a value close to the Coulomb charging energy.
Strain-free GaAs quantum dots (QDs) are fabricated by filling droplet-etched nanoholes in AlGaAs. Using a template of nominally identical nanoholes, the QD size is precisely controlled by the thickness of the GaAs filling layer. Atomic force microscopy indicates that the QDs have a cone-shell shape. From single-dot photoluminescence measurements, values of the exciton emission energy (1.58...1.82 eV), the exciton–biexciton splitting (1.8...2.5 meV), the exciton radiative lifetime of bright (0.37...0.58 ns) and dark (3.2...6.7 ns) states, the quantum efficiency (0.89...0.92), and the oscillator strength (11.2...17.1) are determined as a function of the dot size. The experimental data are interpreted by comparison with an atomistic model.
Self-assembled nanoholes are drilled into (001) AlGaAs surfaces during molecular beam epitaxy (MBE) using local droplet etching (LDE) with Al droplets. It is known that this process requires a small amount of background arsenic for droplet material removal. The present work demonstrates that the As background can be supplied by both a small As flux to the surface as well as by the topmost As layer in an As-terminated surface reconstruction acting as a reservoir. We study the temperature-dependent evaporation of the As topmost layer with in situ electron diffraction and determine an activation energy of 2.49 eV. After thermal removal of the As topmost layer droplet etching is studied under well-defined As supply. We observe with decreasing As flux four regimes: planar growth, uniform nanoholes, non-uniform holes, and droplet conservation. The influence of the As supply is discussed quantitatively on the basis of a kinetic rate model.
Strain-free GaAs cone–shell quantum structures (CSQS) with widely tunable wave functions (WF) are fabricated using local droplet etching (LDE) during molecular beam epitaxy (MBE). During MBE, Al droplets are deposited on an AlGaAs surface, which then drill low-density (about 1 × 10 cm−2) nanoholes with adjustable shape and size. Subsequently, the holes are filled with GaAs to form CSQS, where the size can be adjusted by the amount of GaAs deposited for hole filling. An electric field is applied in growth direction to tune the WF in a CSQS. The resulting highly asymmetric exciton Stark shift is measured using micro-photoluminescence. Here, the unique shape of the CSQS allows a large charge–carrier separation and, thus, a strong Stark shift of up to more than 16 meV at a moderate field of 65 kV/cm. This corresponds to a very large polarizability of 8.6 × 10 eVkV cm2. In combination with simulations of the exciton energy, the Stark shift data allow the determination of the CSQS size and shape. Simulations of the exciton–recombination lifetime predict an elongation up to factor of 69 for the present CSQSs, tunable by the electric field. In addition, the simulations indicate the field-induced transformation of the hole WF from a disk into a quantum ring with a tunable radius from about 10 nm up to 22.5 nm.