Energy storage from renewable sources is possible by chemical procedures, power to gas technology being a possible solution for long-term storage. In this work, CO2 methanation from a sulphur containing gas was studied, taking into account deactivation of the catalysts and a regeneration process. In order to improve the sulphur resistance of a standard nickel (13%) catalyst supported on alumina, transition metals like molybdenum (Mo), iron (Fe), cobalt (Co) or chromium (Cr), in different proportions (from 4 to 8 wt%) were added to the catalyst formulation. The catalyst activity, between 573 and 773 K, at 10 bar, increased when transition metals were added except for Mo in the highest proportion. These bimetallic catalysts presented a similar deactivation resistance than the monometallic catalyst when sulphur was present in the feed. Once H2S was removed from the feed, and the catalysts regenerated with oxygen, only the catalyst containing cobalt recovered up to a 13% methane yield.
In order to reduce greenhouse gas emissions, which are reaching alarming levels in the atmosphere, capture, recovery, and transformation of carbon dioxide emitted to methane is considered a potentially profitable process. This transformation, known as methanation, is a catalytic reaction that mainly uses catalysts based on noble metals such as Ru and, although with less efficiency, on transition metals such as Ni. In order to improve the efficiency of these conventional catalysts, the effect of adding alkaline earth metals (Ba, Ca, or Mg at 10 wt%) and lanthanides (La or Ce at 14 wt%) to nickel (13 wt%), ruthenium (1 wt%), or both-based catalysts has been studied at temperatures between 498 and 773 K and 10 bar pressure. The deactivation resistance in presence of H2S was also monitored. The incorporation of La into the catalyst produces interactions between active metal Ni, Ru, or Ru-Ni and the alumina support, as determined by the characterization. This fact results in an improvement in the catalytic activity of the 13Ni/Al2O3 catalyst, which achieves a methane yield of 82% at 680 K for 13Ni/14La-Al2O3, in addition to an increase in H2S deactivation resistance. Furthermore, 89% was achieved for 1Ru-13Ni/14La-Al2O3 at 651 K, but it showed to be more vulnerable to H2S presence.