Liquid metal fast reactors were considered to be the most promising solution to meet the enormous energy demand in the future. However, corrosion phenomenon caused by the liquid metal, especially in high-temperature lead-bismuth coolant, has greatly hindered the commercialization of the advanced Generation-IV nuclear system. This review discussed current research on the corrosion resistance of structural materials (such as EP823, T91, ODS, and authentic steels) in high-temperature liquid metal served as reactor coolants. The current corrosion resistance evaluation has proved that even for the excellent performance of EP823, the structural material selected in pressurized water reactor is not the ideal material for operation in the high-temperature lead-bismuth eutectic (LBE). Furthermore, the latest coating technologies that are expected to be applied to cladding materials for coolant system were extensively discussed, including Al-containing coatings, ceramic coatings, oxide coatings, amorphous coatings and high-entropy alloy coatings. The detailed comparison summarized the corrosion morphology and corrosion products of various coatings in LBE. This review not only provided a systematic understanding of the corrosion phenomena, but also demonstrated that coating technology is an effective method to solve the corrosion issues of the advanced next-generation reactors.
Al2O3 coatings are the most promising candidate material for mitigating (lead-bismuth eutectic) LBE corrosion at elevated temperatures, but preventing inward diffusion of Pb, Bi, and O for the ceramic coating remains a critical challenge. Here, we have fabricated an amorphous Al2O3 coating with an ultra-dense structure by continuous high-power magnetron sputtering (C-HPMS). After LBE corrosion at 550 °C for 2000 h, nanocavities induced by the phase transformation from amorphous to γ-Al2O3 provide the diffusion path for Fe, O, Pb, and Bi in which the corrosion products, such as Fe3O4, PbO2, or their mixed oxides, form. Furthermore, the diffusion of Pb to the substrate and Cr segregation at the interface between the coating and substrate are observed for the sample exposed to LBE at 550 °C for 4000 h. Additionally, the hardness and interface bonding strength are enhanced after LBE corrosion. Moreover, pit corrosion was found to be the main failure mode of coating, and pits that merged with each other induced large area failure at a temperature of 650 °C. The corrosion mechanism of Al2O3 includes element diffusion, phase transformation, and chemical reaction. This work not only provides a deep understanding of the corrosion mechanism of amorphous Al2O3 coatings, but also shows the optimization method on the corrosion resistance of Al2O3 coating.
The corrosion behavior of alumina-forming austenitic (AFA) stainless steels with different Nb additions in a supercritical carbon dioxide environment at 500 °C, 600 °C, and 20 MPa was investigated. The steels with low Nb content were found to have a novel structure with a double oxide as an outer Cr2O3 oxide film and an inner Al2O3 oxide layer with discontinuous Fe-rich spinels on the outer surface and a transition layer consisting of Cr spinels and γ’-Ni3Al phases randomly distributed under the oxide layer. Oxidation resistance was improved by accelerating diffusion through refined grain boundaries after the addition of 0.6 wt.% Nb. However, the corrosion resistance decreased significantly at higher Nb content due to the formation of continuous thick outer Fe-rich nodules on the surface and an internal oxide zone, and Fe2(Mo, Nb) laves phases were also detected, which prevented the outward diffusion of Al ions and promoted the formation of cracks within the oxide layer, resulting in unfavorable effects on oxidation. After exposure at 500 °C, fewer spinels and thinner oxide scales were found. The specific mechanism was discussed.