Designing phosphors that are excited by blue light is extraordinarily important for white light-emitting diodes (w-LEDs). In the present study, a new Ruddlesden–Popper type of SZO:xEu3+ (x = 0.01~0.10) phosphors was developed using solid-state reactions. Interestingly, a Eu3+ doping-induced phase transformation from the Sr3Zr2O7 (cubic) to the SrZrO3 (orthorhombic) phase was observed, and the impact of the occupied sites of Eu3+ ions on the lifetime of Sr3Zr2O7:xEu3+ phosphors is discussed in detail. Diffuse reflectance spectroscopy results showed that the band gap of SZO:xEu3+ phosphors gradually increased from 3.48 eV for undoped Sr3Zr2O7 hosts to 3.67 eV for SZO:0.10Eu3+ samples. The fluorescence excitation spectrum showed that ultraviolet (300 nm), near-ultraviolet (396 nm) and blue light (464 nm) were all effective excitation pump sources of Sr3Zr2O7:xEu3+ phosphors, and the strongest emission at 615 nm originated from an electric dipole transition (5D0→7F2). CIE coordinates moved from orange (0.5969, 0.4267) to the reddish-orange region (0.6155, 0.3827), and the color purity also increased. The fabricated w-LED was placed on a 460 nm chip with a mixture of YAG:Ce3+ and SZO:0.1Eu3+ samples and showed “warm” white light with a color rendering index (CRI) of 81.8 and a correlation color temperature (CCT) of 5386 K, indicating great potential for application in blue chip white LEDs.
A new tellurium polyoxomolybdate hydrate (NH4)2K2TeMo6O22·2H2O was synthesized via the hydrothermal reaction method at 190 °C. The compound crystallizes in a one-dimensional tellurium polymolybdate [TeMo6O22]4− chain structure. The anionic polymeric chain is composed of Mo6O22 hexamers bridged together through sharing four corner oxygen atoms on the electron lone-paired TeO4 group. The Mo6O22 hexamer cluster is assembled from six distorted MoO6 octahedra in an edge-sharing manner. The ammonium and potassium cations distribute around the [TeMo6O22]4− chains and separate them from each other and maintain the charge balance. The thermal stability and optical properties of the compound were also investigated. The optical absorption data reveal that the compound is a wide band semiconductor with an optical band gap of 3.4 eV.
Polymorphic transition, as an interesting phenomenon in many fields of materials chemistry, can take place upon heating, pressure, or ion doping. Herein, we achieved hexagonal to monoclinic phase transition of Tb3+ doped CePO4 (CePO4:Tb3+) nanocrystal through a simple and convenient ball milling method, but with reduced photoluminescence. The decrease in luminescence may be due to the partial oxidation of Ce3+ to Ce4+ during the ball milling process, as well as the decrease in crystal symmetry in monoclinic phase.