Amorphous calcium phosphate (ACP), a postulated precursor in the formation of biological hydroxyapatite, has been evaluated as a filler phase in bioactive polymeric composites that utilize dental monomers to form the matrix phase on polymerization. In addition to excellent biocompatibility, these composites provided sustained release of calcium and phosphate ions into simulated saliva milieus. In an effort to enhance the physicochemical and mechanical properties and extend the utility of remineralizing ACP composites to a greater variety of dental applications, we have focused on: a) hybridizing ACP by introducing silica and/or zirconia, b) assessing the efficacy of potential coupling agents, c) investigating the effects of chemical structure and compositional variation of the resin matrices on the mechanical strength and ion-releasing properties of the composites, and d) improving the intrinsic adhesiveness of composites by using bifunctional monomers with an affinity for tooth structure in resin formulations. Si- and Zr-modified ACPs along with several monomer systems are found useful in formulating composites with improved mechanical and remineralizing properties. Structure-property studies have proven helpful in advancing our understanding of the remineralizing behavior of these bioactive composites. It is expected that this knowledge base will direct future research and lead to clinically valuable products, especially therapeutic materials appropriate for the healing or even regeneration of defective teeth and bone structures.
This study explores how the resin composition/structure affects the physicochemical properties of copolymers and their amorphous calcium phosphate (ACP)-filled composites. A series of photo-polymerizable binary and ternary matrices are formulated utilizing 2,2-bis[ p-(2'-hydroxy-3'methacryloxypropoxy)phenyl]propane, 2,2-bis[ p-(2'-methacryloxypropoxy)phenyl]-propane (EBPADMA), or a urethane dimethacrylate as base monomers, and triethylene glycol dimethacrylate or hexamethylene dimethacrylate (HmDMA) with or without 2-hydroxyethyl methacrylate (HEMA) as diluent monomer. Unfilled copolymers and composites filled with 40% by mass zirconia-hybridized ACP are evaluated for biaxial flexure strength (BFS), degree of conversion (DC), mineral ion release, polymerization shrinkage (PS), and water sorption (WS). The average DC values are 82—94% and 74—91% for copolymers and composites, respectively. Unrelated to the resin composition, the PS values of composites are up to 8.4 vol. % and the BFS values of wet composite specimens are on average 51 ± 8 MPa. The maximum WS values attained in copolymers and composites reach 4.8 mass%. Inclusion of hydrophobic HmDMA monomer in the matrices significantly reduces the WS. The levels of Ca and PO4 released from all types of composites are significantly above the minimum necessary for the re-deposition of apatite to occur. Elevated Ca, and to a lesser extent PO4 release, is observed in HEMA-containing, ternary EBPADMA formulations. Further resin reformulations may be needed to improve the PS of composite specimens. Poor dispersion of `as-synthesized' ACP within the composite contributes to their inferior mechanical performance.
16 November 2001 in Journal of Biomedical Materials Research