The fracture mechanics-based IBESS approach is applied to the determination of FAT classes of butt welds with crack initiation along the weld toe. The aim is an investigation of the effect of the geometrical parameters toe radius, flank angle, reinforcement and secondary notches such as roughness or undercuts. The influence of these parameters is discussed both individually and in combination; however, excluding statistical distributions of them and the material data. The results, when compared with conventional FAT classes for butt welds, are encouraging with respect to a potential contribution of IBESS to the discussion of more advanced quality criteria for welds. To that purpose, demands for further research are proposed.
The paper provides an overview on the results of a German cluster project on the use of fracture mechanics to the determination of the fatigue strength of weldments with fatigue cracks originating at the weld toes. The approach includes (a) a concept for short crack propagation for which the common ΔK concept is not applicable and the crack closure effects are still being gradually build-up, (b) a method for determining fatigue life relevant initial crack sizes as they are needed in any fracture mechanics analysis and (c) multiple cracking and crack coalescence at load levels higher than the endurance limit. The analyses are stochastically performed. Both, the endurance limit and the finite life branch of the S-N curve are determined. Besides a brief introduction into the approach, validation examples are presented. These comprise different weldment types (butt welds, cross joints and longitudinal stiffened plates), two steels (S355NL and S960QL) of quite different strengths, different weld geometries due to different welding techniques (WIG, MAG), as-welded and stress relieved welds and different stress ratios varying from R = -1 to R = 0.5.
The safe fatigue design of metallic components fabricated by additive manufacturing (AM) is still a largely unsolved problem. This is primarily due to (a) a significant inhomogeneity of the material properties across the component; (b) defects such as porosity and lack of fusion as well as pronounced surface roughness of the as-built components; and (c) residual stresses, which are very often present in the as-built parts and need to be removed by post-fabrication treatments. Such morphological and microstructural features are very different than in conventionally manufactured parts and play a much bigger role in determining the fatigue life. The above problems require specific solutions with respect to the identification of the critical (failure) sites in AM fabricated components. Moreover, the generation of representative test specimens characterized by similar temperature cycles needs to be guaranteed if one wants to reproducibly identify the critical sites and establish fatigue assessment methods taking into account the effect of defects on crack initiation and early propagation. The latter requires fracture mechanics-based approaches which, unlike common methodologies, cover the specific characteristics of so-called short fatigue cracks. This paper provides a discussion of all these aspects with special focus on components manufactured by laser powder bed fusion (L-PBF). It shows how to adapt existing solutions, identifies fields where there are still gaps, and discusses proposals for potential improvement of the damage tolerance design of L-PBF components.