The utilisation of rice husk ash (RHA) as an aluminosilicate source in fire-resistant coating could reduce environmental pollution and can turn agricultural waste into industrial wealth. The overall objective of this research is to develop a rice-husk-ash-based geopolymer binder (GB) fire-retardant additive (FR) for alkyd paint. Response surface methodology (RSM) was used to design the experiments work, on the ratio of RHA-based GB to alkyd paint. The microstructure behaviour and material characterisation of the coating samples were studied through SEM analysis. The optimal RHA-based GB FR additive was formulated at 50% wt. FR and 82.628% wt. paint. This formulation showed the result of 270 s to reach 200 °C and 276 °C temperature at equilibrium for thermal properties. Furthermore, it was observed that the increased contents of RHA showed an increment in terms of the total and open porosities and rough surfaces, in which the number of pores on the coating surface plays an important role in the formation of the intumescent char layer. By developing the optimum RHA-based GB to paint formulation, the coating may potentially improve building fire safety through passive fire protection.
1 February 2017 in International Journal of Materials, Mechanics and Manufacturing
This paper represents the performance of a natural fiber cycling helmets in an oblique impact with a simulated road surface. The linear accelerations and impact energy of a head form that weight four kilogram were measured and calculated. Helmet standards require helmets to be designed only to survive a simple drop test onto an anvil. The maximum permitted deceleration of the dropped head form is typically 300g, which is equivalent to an impact velocity of 20 km/h (12.5 mph). Two helmets being tested suspended onto a guided drop-table in the particular desired impact orientation. Just before impact, the test object is released from suspension so it can move unrestrained thereafter. The main advantages of this process are that the object is free to move naturally during impact which provides for more realistic drop-testing. For oblique impact test, all helmets that tested pass the requirement that is set by EN1078:2007 by having linear acceleration below than 250g in a free fall 1.5 m platform. By comparing the linear acceleration resultant with an existing cycling helmet in the market Kabuto Aero SL, flax aero helmet shows 11.82% linear acceleration resultant loss with 214.16g. Kenaf helmet recorded 168.48g with 30.63% linear acceleration resultant loss from the Kabuto helmet and 21.33% linear acceleration resultant loss from the Flax helmet.