The demand for heat-resistant steel has increased owing to its utility in numerous devices that must withstand high steam pressures and high temperatures, such as turbine rotors and blades in ultra-supercritical power plants. It is inevitable to join heat-resistance steel part by welding method, so it is important to maintain the toughness of the weld metals. In this study, the microstructure, low-temperature impact toughness, and fracture surface of as-welded and post-weld heat treatment (PWHT) of 2.25Cr-1Mo-0.25V weld metal were investigated. The microstructures of the as-welded and PWHT specimens are granular bainite and ferrite, respectively. This work revealed the relationship between effective microstructure nearby crack initiation origin and low temperature impact toughness for both the as-welded and PWHT specimens. The evolution of the microstructure and prior austenite was then investigated using confocal laser scanning microscopy (CLSM) to observe the formation of coarse ferrite grain structures. A suggestion for enhancing the low-temperature toughness was provided based on the effect of adjusting Mn content and forming acicular ferrite.
Oxide dispersion strengthened ferritic steel is considered an important structural material in fusion reactors due to its excellent resistance to radiation and oxidation. Fine and dispersed oxides can be introduced into the matrix via the powder metallurgy process. In the present study, large grain sizes and prior particle boundaries (PPBs) formed in the FeCrAlY alloy prepared via powder metallurgy. Thermo-mechanical treatment was conducted on the FeCrAlY alloy. Results showed that microstructure was optimized: the average grain diameter decreased, the PPBs disappeared, and the distribution of oxides dispersed. Both ultimate tensile strength and elongation improved, especially the average elongation increased from 0.5% to 23%.
22 January 2022 in Journal of Materials Engineering and Performance
Fe-Ni-Cr austenitic alloys are widely used in hydrogen environments as structural materials. Their weld normally shows higher hydrogen-embrittlement sensitivity than the base metal, endangering large-scale applications. Herein, by using electron microscopy and numerical calculations, the influence of applied load on the fracture mode of hydrogen-embrittled JBK-75 alloy weldment is revealed and correlated with a competition between hydrogen-prompted intergranular decohesion (HPID) and hydrogen-enhanced localized plasticity (HELP). Therefore, independent of the load levels, the weld featuring a lower strength and smaller grain sizes is always more vulnerable to hydrogen embrittlement than the base metal.
The high tensile strength and irradiation resistance of oxide dispersion strengthened (ODS) ferritic steels is attributed to the ultrafine and dispersed oxides within the matrix. The high content of oxygen and yttrium is critical for the formation of dense Y-rich oxides. However, only few studies have reported the effect of oxygen content on the microstructure and mechanical properties of ODS steels. Herein, we employed gas atomization reactive synthesis to prepare pre-alloy powders and then hot isostatic pressing (HIP) to consolidate two 22Cr-5Al ODS steels with different oxygen content. Our results showed Y-rich precipitates at and near grain boundaries of the as-HIPed alloys. Moreover, with the oxygen content increasing from 0.04 to 0.16 wt%, more precipitates precipitated in the as-HIPed alloy, and the ultimate tensile strength of the alloy was improved. However, increasing the oxygen content to 0.16 wt% led to formation of stripe and chain precipitates at and near grain boundaries, which caused a partial intergranular fracture of the as-HIPed alloy.