Within the Waste2Fuel project, innovative, high-performance, and cost-effective fuel production methods are developed to target the “closed carbon cycle”. The catalysts supported on different metal oxides were characterized by XRD, XPS, Raman, UV-Vis, temperature-programmed techniques; then, they were tested in CO2 hydrogenation at 1 bar. Moreover, the V2O5 promotion was studied for Ni/Al2O3 catalyst. The precisely designed hydrotalcite-derived catalyst and vanadia-promoted Ni-catalysts deliver exceptional conversions for the studied processes, presenting high durability and selectivity, outperforming the best-known catalysts. The equilibrium conversion was reached at temperatures around 623 K, with the primary product of reaction CH4 (>97% CH4 yield). Although the Ni loading in hydrotalcite-derived NiWP is lower by more than 40%, compared to reference NiR catalyst and available commercial samples, the activity increases for this sample, reaching almost equilibrium values (GHSV = 1.2 × 104 h–1, 1 atm, and 293 K).
The effect of La content and its incorporation route on physicochemical properties of ZnO/Zn(Al,La)2O4 or La2O3–ZnO/ZnAl2O4 mixed oxides with a spinel structure obtained from ZnAlLa Layered double hydroxides (LDHs) or ex-ZnAl LDH materials was investigated. The heterostructural nanocomposites with the similar Zn/Al molar ratio and varied La content were prepared by two techniques: via co-precipitation and thermal treatment of ZnAlLa LDHs at 500 °C or via incipient wetness impregnation of ex-ZnAl LDHs with aqueous solutions of lanthanum nitrate and subsequent thermal treatment. The obtained series of materials were characterized by the following techniques: X-ray fluorescence (XRF), N2 adsorption (BET), X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FT-IR), thermogravimetric analysis with evolved gas analysis (TG/DTG/EGA), scanning transmission electron microscopy (STEM) energy-dispersive X-ray spectroscopy (EDS), high-resolution transmission electron microscopy (HRTEM) and Fourier-transform infrared spectroscopy (FFT). The evaluation of activity toward the high-temperature water gas shift (HT-WGS) within the temperature range of 350–420 °C was carried out on the basis of rate constant measurements in the kinetic mode using a differential reactor. The co-precipitation technique allowed for a better distribution of La in bulk and on the spinel surface than in case of lanthanum incorporation via impregnation. ZnO/Zn(Al,La)2O4 or La2O3–ZnO/ZnAl2O4 mixed oxides were characterized by moderate activity in the HT-WGS reaction. The results reveal that introduction of lanthanum oxide over 2.4–2.8 wt% induces the phase separation of the ZnAl2O4 spinel, forming ZnO on the ZnAl2O4 spinel surface.
A set of ex-ZnAl-LDHs catalysts with a molar ratio of Zn/Al in the range of 0.3–1.0 was prepared using co-precipitation and thermal treatment. The samples were characterized using various methods, including X-ray fluorescence spectroscopy (XRF), X-ray photoelectron spectroscopy (XPS), X-ray powder diffraction (XRD), Fourier transform infrared spectroscopy FT-IR, N2 adsorption, Temperature-programmed desorption of CO2 (TPD-CO2) as well as Scanning electron microscopy (SEM-EDS). Catalyst activity and long-term stability measurements were carried out in a high-temperature water–gas shift (HT-WGS) reaction. Mixed oxide catalysts with various Zn/Al molar ratios decorated with potassium showed high activity in the HT-WGS reaction within the temperature range of 330–400 °C. The highest activity was found for the Zn/Al molar ratio of 0.5 corresponding to spinel stoichiometry. However, the catalyst with a stoichiometric spinel molar ratio of Zn/Al (ZnAl_0.5_K) revealed a higher tendency for surface migration and/or vaporization of potassium during overheating at 450 °C. The correlation of the activity results and TPD-CO2 data show that medium basic sites enhance the progress of the HT-WGS reaction.