Composite ZrB2–MoSi2 coating modified by Y2O3 and Al was prepared by a new multi-chamber detonation accelerator (MCDS) on carbon/carbon composites. Postdeposition heat treatment of the samples at 1500 °C for 1 and 6 h was carried out in air. The effect of heat treatment on the microstructure and phase composition of the ZrB2–MoSi2 coating was investigated by scanning electron microscopy and X-ray diffraction phase analysis. The as-sprayed coating presented as a dense lamellar structure, composed of m-ZrO2, t-ZrO2, some hexagonal ZrB2, and cubic Al phases. The m-ZrO2, c-ZrO2, and h-(α-Al2O3) formed at 1500 °C. The coatings after heat treatment (1 and 6 h) exhibited a structure without cracks. The porosity (~1%) of the coating did not change after heat treatment. Thin, continuous, silica-rich film covered the surfaces of ZrO2 and Al2O3 particles, and could have played a role during heat treatment by acting as a grain lubricant for particle rearrangement.
Surface topography and residual stresses in surface layers of α + β titanium alloy Ti6Al4V textured by 1030-nm, 320-fs-laser pulses were studied by scanning electron microscopy and X-ray diffraction analysis. It was found that multipulse laser processing leads to the formation of laser-induced periodic surface structures (LIPSS) on the surface of Ti6Al4V alloy. XRD studies showed that depending on the laser pulse fluence, both tensile and compressive residual stresses are formed in thin near-surface layers.
The problem of creating and implementing high-temperature coatings for the protection of carbon–carbon (C/C) composites remains relevant due to the extremely low or insufficient heat resistance of C/C composites in an oxygen-containing environment. In the present work, detonation spraying was used for preparing new ZrB2–35MoSi2–10Al coatings on the surface of C/C composites without a sublayer. As a stabilizer of high-temperature modification of zirconia, and to increase the wettability of the surface of C/C composites, 5 wt.% Y2O3 and 10 wt.% Al were added to the initial powder mixture, respectively. The structure of the as-sprayed coating presents many lamellae piled up one upon another, and is composed of hexagonal ZrB2 (h- ZrB2), tetragonal MoSi2 (t-MoSi2), monoclinic ZrO2 (m-ZrO2), tetragonal ZrO2 (t-ZrO2), monoclinic SiO2 (m-SiO2), and cubic Al phases. The oxidation behavior and microstructural evolution of the ZrB2–35MoSi2–10Al composite coating were characterized from RT to 1400 °C in open air. During oxidation at 1400 °C, a continuous layer of silicate glass was formed on the coating surface. This layer contained cubic ZrO2 (c-ZrO2), m-ZrO2, and small amounts of mullite and zircon. The results indicated that a new ZrB2–35MoSi2–10Al composite coating could be used on the surface of C/C composites as a protective layer from oxidation at elevated temperatures.