To analyze the effect of nano-solid particles on the mechanical properties of shear thickening fluid (STF) and its Kevlar composite fabric. In this study, nano-silica and polyethylene glycol (PEG 200) were used as dispersed and continuous phases. Nano-graphite and nano-diamond particles were used as additives to prepare STF and Kevlar composite fabric. Study the friction characteristics and rheological characteristics of STF at different temperatures. Explore the STF’s mechanical response under transient high-speed impact conditions through the split Hopkinson pressure bar experiment. The mechanical properties of STF-Kevlar fabric are studied through yarn pull-out test and burst experiments. The experimental results show that the intermolecular repulsive force of STF is enhanced under a high-temperature environment, and shear thickening effect is reduced. Nano-diamond particles strengthen the contact coupling force and contact probability between the particle clusters, so that the maximum viscosity of the system reaches 1679 Pa s, the thickening ratio reaches 318 times, and the rheological properties of the shear thickening fluid are improved. The results of the SHPB experiment show that the STF can complete a dynamic response within a 50–75 µs time range, and the maximum stress can reach 78 MPa. The bullet’s incident kinetic energy is not only transformed into thermal energy and phase change energy of solid-liquid conversion, but also into frictional energy between particles. The mechanical experiments of STF-Kevlar composite fabrics show that the tensile force value of STF5-Kevlar is the largest (10.3 N/13.5 N), and the tensile force of neat Kevlar was the smallest (4.3 N/4.9 N). The maximum bearing capacity (0.3 kN) and absorption energy (51.8 J) of Neat Kevlar are less than those of STF1-Kevlar (3.2 kN, 116.7 J) and STF3-Kevlar (1.9 kN, 88.2 J), and STF5-Kevlar (4.7 kN, 143.3 J). Fabric’s failure mode is converted from partial yarn extraction to overall deformation and rupture of the fabric. Therefore, by changing the solid additives’ parameters, the STF and the composite fabric’s mechanical properties can be effectively controlled, which provides a reference for preparing the STF and fabric composite materials.
This paper analyzed the influence of various components and the external environment on the rheological properties of shear thickening fluid (STF). The single-factor experimental study was carried out with the silica particle size, the mass fraction of silica particles, the continuous phase’s average molecular weight, and the temperature as the influencing factors. Obtain the influence of various factors on the initial viscosity, critical shear rate, thickening period and thickening ratio of STF samples. According to the crossover relationship between the shear stress and the intermolecular force when the shear thickening occurs, the STF’s critical shear rate criterion is constructed. By introducing the mechanical balance between small molecules, the relationship between the particles’ volume fraction and the distance between particles in the suspension system is established. The influencing factors and formulas of the STF’s critical shear rate and shear capacity are deduced, which supports the conclusions obtained in the single-factor experiment. Based on the single-factor experiment conclusion, the mass fraction of silica particles, the average molecular weight of the continuous phase and the temperature are used as the influencing factors, and the critical shear rate, shear thickening ratio and maximum viscosity are the responses indicators. According to the Box-Behnken response surface methodology (RSM) design, 15 analysis experiments with three factors and three levels are carried out. Obtain the rheological characteristics of the STF and regression equation between each factor, based on the three-dimensional response surface graph and F-value in ANOVA result. We found that among the interaction effects, the interaction between the continuous phase’s average molecular weight and the temperature has the most significant impact on the critical shear rate of the STF. The interaction between the silica particles’ mass fraction and the continuous phase’s average molecular weight significantly impacts the shear thickening ratio of the STF. The interaction between silica particles’ mass fraction and the temperature has the most significant impact on the maximum viscosity of the STF. Finally, according to the response surface methodology experimental results and ideal STF rheological characteristics standard in engineering applications, when the mass fraction of silica particles is 35%, the average molecular weight of the continuous phase is 387, and the temperature is 20 °C. The critical shear rate of the STF system is 5.84 1/s, the shear thickening ratio is 102.8, and the peak viscosity is 1191.7 Pa·s, reaching the optimal theoretical value within the value scope.
In this paper, high density rigid polyurethane foam is used as sandwich skeleton and shear thickening fluid as material core. A shear thickening fluid/polyurethane sandwich structure with light impact resistance was designed and fabricated. High strain rate impact test was carried out. It was found that STF-2/PU reached the peak load of 4978N in 13 ms after receiving 20 J impact energy, and the energy absorption ratio was as high as 43%. The shear thickening fluid/polyurethane honeycomb sandwich foam prepared by secondary foaming process has stable structure and can effectively absorb impact energy to achieve good protection effect.
Magnetorheological fluids (MRFs) exhibit different wear performance when nanoparticles with different hardness are added. In this study, three solid particles with different hardness are considered to study the variation in MRF performance. The friction and wear properties of the MRF are measured by using a four-ball friction and wear tester, and the surface of the steel ball was observed using a three-dimensional white light interferometer. Also, the rheological properties of MRF are tested by using an Anton-Paar rheometer. The results show that the addition of graphite yields a stable friction process and does not degrade the rheological properties of MRF. Nano-diamond increases the shear yield strength and reduces the wall slip to a greater extent. However, the wear is more serious in this case. Copper particles are unstable, and their surface activity is too high to get adsorbed on the surface of iron powder aggravating the settlement rate. The above three MRFs with different kinds of nano-particles present a more regular grinding spot, and the nano-particles have a certain repair function to the surface.