Arc-melting (AM) as a primary method for casting high entropy alloys (HEAs) ensures rapid alloy screening with minimal material input, high cost-effectiveness, and high cooling rates. However, the limitations of AM on a laboratory scale, particularly its constrained sample size and the necessity for remelting steps to ensure homogeneity, hampers thorough mechanical and functional testing of bulk materials. Therefore, this study features a comparative analysis between AM and vacuum induction-melting (VIM) techniques for High Entropy Shape Memory Alloys (HE-SMAs) production, focusing on the senary alloy Ti16.6Zr16.6Hf16.6Co10Ni20Cu20, known for its potential functional applications and high sensitivity to material inhomogeneity. The alloy’s composition, including high-melting point elements like Hf, Ti and Zr, makes it a well-suited candidate for assessing the capabilities of VIM in producing homogeneous bulk materials. The employment of binary pre-alloys in both AM and VIM processes reduced the necessity for remelting steps and ensured better initial quality for subsequent heat treatments. A homogenization treatment at 900 °C for 100 h of an AM-produced senary alloy showed only slight improvements compared to the same alloy produced via VIM, largely due to the slow diffusion of the larger Hf and Zr atoms from the dendrites into the solid solution. This suggests that VIM can achieve comparable levels of homogenization in substantially less time than required for AM-treated samples. The findings finally indicate that by using VIM, when combined with binary pre-alloys, one achieves more homogeneous alloys with reduced heat-treatment time, making it a viable method for HE-SMA production.
The influence of pre-strain on the very-low-cycle loading behavior as occurring, for example during roller leveling of sheet metals, is not yet fully understood. A key factor in this context is the stiffness of the material and its changes upon processing. To study the general mechanical property changes during low-cycle loading with small amplitudes for a wide variety of metals, sheet samples of mild steel DC01, pure copper CU-DHP and α-titanium are subjected to low-cycle tension–compression tests. The general influences of pre-strain and the applied strain amplitude are investigated regarding material hardening and changes in the elastic properties. It is shown that all tested materials feature changes in the Bauschinger behavior during cycling. The apparent elastic modulus of the materials decreases with increasing accumulated plastic strain, and the evolution depends on the strain amplitude and the pre-strain. For all three materials, changes in technical springback are present and depend on the loading history.
For studies of the interface zone of metallic composites with significantly differing mechanical properties across the interface, high-quality sample preparation is paramount. In particular, the analysis of the composition or geometric characteristics of intermetallic phases close to the interface requires a preparation specifically adapted to the actual sample. In the present study, the combination of ion beam processing and a conventional metallographic preparation routine is investigated. It is shown that by utilizing a suitable combination of metallographic and ion beam processing routines, the interface zone of metallic composites can be prepared specifically targeted to a given analytical task. Especially for material combinations with largely differing mechanical properties of the base materials, ion beam processing can greatly improve the sample preparation quality.
One possibility to increase the interface strength of cold roll bonded materials is the application of a thin intermediate layer. In the present study, a tin coating was employed to strengthen the interface formed between cold roll bonded steel sheets, and the impact of subsequent heat treatment on the resulting bonding strength was investigated. To increase the bond strength by diffusion, the tin-coated steel bonds underwent heat post-treatment between temperatures of 150 °C and 300 °C for different dwell times. The results demonstrate that the use of tin as an active intermediate layer increases the bond area established. Moreover, the thin tin coating results in the formation of an active intermediate layer that directly takes part in the joining process by establishing a reactive link between the two substrates. A subsequent heat treatment further affects the bond strength by diffusion of tin at the interface.