Carbon nanotubes (CNTs) coated with SiC coating was successfully prepared by pyrolysis of polycarbosilane (PCS) used as a precursor. The function of pyrolysis temperature on the oxidation resistance and the dielectric properties of CNTs/SiC were studied in X-band. The results demonstrate that the obtained dense SiC film can prevent the oxidation of CNTs when the pyrolysis temperature reaches 600 °C. Correspondingly, after heat treatment is at 400 °C for 200 h, the mass loss of P-600 is less than 1.86%, and the real and imaginary parts of the dielectric constant nearly keep constant (ε′ from 14.2 to 14, and ε″ from 5.7 to 5.5). SiC-coated CNTs have a better oxidation resistance than pristine CNTs. Therefore, this work, with a facile preparation process, enhances the oxidation resistance of CNTs at high temperature for a long time and maintains a stable dielectric property, which means CNTs/SiC composites can be good candidates for applications in the field of high-temperature absorbers.
Carbon nanotube (CNT)-reinforced Y2O3/ZrB2 ceramics were fabricated via planetary ball milling and atmospheric-pressure plasma spraying for the first time. The phase composition, micromorphology, and electromagnetic (EM) wave absorption performance of the Y2O3/ZrB2/CNT hybrid was investigated from 8.2 to 12.4 GHz. Both the real and imaginary parts of the complex permittivity were enhanced as the ZrB2 and CNT content increased. The Y2O3/ZrB2/CNT hybrids corresponded to a ZrB2 content of 15 wt.%, and the CNT content was 2 wt.% and showed an exceptional EM wave absorption capability, with a minimum reflection loss of −25.7 dB at 1.9 mm thickness, and the effective absorption band was in a full X-band. These results indicate that an appropriate CNT or ZrB2 content can tune the complex permittivity and absorption performance of the Y2O3/ZrB2/CNT ceramics.
Rubber-based conductive composites are widely used in sensors, wearable electronic devices and electromagnetic fields. In this work, by using the two-roll milling and hot-pressing process, chopped glass fiber (CGF) and graphene (Gr) as additives, and acrtlinitrile-brtadiene rubber (NBR) as the matrix, a series of anisotropic flexible rubber-based composites were prepared. Using this preparation method, both CGF and Gr additives were directly arranged in the material. When the content of CGF was 1 wt.%, the tensile strength in both the T and W directions of the material reached 27 MPa and 28 MPa, respectively. When the content of CGF was fixed at 1 wt.% and Gr was 1.5 wt.% and the elongation at break in both directions reached 328% and 347%. By focusing on the comparison of the dielectric differences in the T and W directions in the X band, it was found that the directional arrangement of the additives led to differences in the dielectric properties.