The present study aimed at assessing mechanical and durability characteristics of ground granulated blast furnace slag (GGBS)-based geopolymer composites at 5%, 10%, 15%, 20%, 25%, and 30% replacement proportion of silica fume at 12 molarity of NaOH. Mechanical properties were assessed using compression and tension tests, whereas durability characteristics were evaluated using ultrasonic pulse velocity test (UPV), acid test, and rapid chloride permeability test (RCPT), and water absorption (WA) test. Additionally, reduction in mass and strength were also determined due to the acid action on the developed composites. A correlation of compressive strength was also established with the splitting tensile strength, UPV, RCPT, and WA. The presence of silica fume and high NaOH concentration in GPC tends to improve the mechanical strength up toa certain level. UPV values obtained were falling in the range of medium to good category. Chloride ion penetration and water absorption values were reduced by around 23% and 26%, respectively, at 10% silica fume replacement. Mass loss and strength loss were reduced as the % of silica fume increased. A good correlation of compressive strength was obtained with tensile strength, UPV, and RCPT with a coefficient of determination of 0.9681, 0.9665, and 0.9208, respectively. Poor correlation was obtained between compressive strength and water absorption.
Alkali activation of ground-granulated blast-furnace slag (GGBS) and calcined clay is a long-term solution for recycling industrial waste into geopolymer composites. The aim of this investigation is to develop ground granulated blast furnace slag (GGBS) and calcined clay based geopolymer mortar. Both GGBS and calcined clay are alumino silicates that are activated using alkaline activator. 8 M sodium hydroxide solutions are used to develop the alkaline activator. Consistency, setting time and compressive strength of geopolymer were investigated in respect to mixture proportioning and curing conditions at the age of 3, 7, 28 days. The percentage of calcined clay, GGBS, fines content and alkaline activator solution content were all examined process parameters. The experimental results showed that the consistency and setting time were enhanced with increased the percentage of calcined clay in geopolymer mortar. The maximum compressive strength is attained at 100% used of GGBS in mortar mix while increasing the percentage of calcined clay replaced with ggbs in the mortar mix compressive strength was reduced.