Two primary engineering challenges are en route to fabricating high-performance flexible stainless-steel based Cu(In,Ga)(S,Se)2solar cells; Growing absorbers without contamination from the substrate, and providing alkali dopants to the absorber. The former is chiefly addressed by introducing a barrier layer, and the latter by post-deposition treatment or including dopant-containing layers in the stack. Here we organize these solutions and different approaches in an accessible scheme. Additionally, reports on interaction between contamination and alkali elements are discussed, as is the impact of barrier layer properties on the interconnect technology. Lastly, we make recommendations to consolidate the multitude of sometimes inharmonious solutions.
Cu(In,Ga)(S,Se)2 absorbers with a bandgap in the near-infrared region are ideal candidates for a bottom cell in multi-junction solar cell architectures. In flexible and lightweight form factors, such devices could help power many applications through integrated solar cells. Here, we show the use of a two-step method to synthesize Cu(In,Ga)(S,Se)2, with a bandgap between 1.00 and 1.13 eV, on bendable ultra-thin glass, with minority carrier lifetimes approaching 100 ns, in a homogenous and repeatable fashion. We also report on conventional and alternative device fabrication methods with very low waste and toxicity footprints. Champion solar cells are fabricated based on absorbers with a graded bandgap between 1.05 and 1.1 eV, and an open circuit voltage approaching 600 mV. Our results show a way for scalable fabrication of all thin-film, flexible tandem solar cells, by means of industrially relevant processing steps in a low cost and sustainable fashion.
Pure sulfide CIGS solar cells are interesting candidates for standalone solar cells or top cells in a tandem configuration. To understand the limits and improve the power conversion efficiency of these devices, a comprehensive approach aimed at composition, interface, and process engineering should be employed. Here, the latter was explored. Using a two-step fabrication technique and one-variable-at-a-time methodology, we found the four processing factors affecting the absorber the most. While two were already backed by the previous literature, we found new and statistical evidence for two other important factors as well. The impact of alkali barrier diffusion was also established with statistical significance and under various processing conditions. Furthermore, the absorber roughness for samples without a barrier indicated a significant negative linear correlation with the devices’ efficiency. This contribution could aid engineers in more efficient process designs.
5 August 2025 in ACS Applied Materials & Interfaces