The scope of this study includes modeling and experimental investigation of sulfide stress cracking (SSC) of high-strength carbon steel. A model has been developed to predict hydrogen permeation in steel for a given pressure and temperature condition. The model is validated with existing and new laboratory measurements. The experiments were performed using C-110 grade steel specimens. The specimens were aged in 2% (wt.) brine saturated with mixed gas containing CH4, CO2, and H2S. The concentration H2S was maintained constant (280 ppm) while varying the partial pressure ratio of CO2 (i.e., the ratio of partial pressure of CO2 to the total pressure) from 0 to 15%. The changes occurring in the mechanical properties of the specimens were evaluated after exposure to assess material embrittlement and SSC corrosion. Besides this, the cracks developed on the surface of the specimens were examined using an optical microscope. Results show that the hydrogen permeation, and subsequently SSC resistance, of C-110 grade steel were strongly influenced by the Partial Pressure Ratio (PPR) of CO2 when the PPR was between 0 and 5%. The PPR of CO2 had a limited impact on the SSC process when it was between 10 and 15 percent.
1 July 2026 in Green Technologies and Sustainability
Despite decades of investigation, a complete understanding of CO2 corrosion under complex environmental and operational conditions remains challenging. The stability and protective properties of corrosion-product scales across a wide range of service conditions are also poorly understood, limiting the effectiveness of corrosion management strategies. This review critically assesses CO2 corrosion behavior under diverse conditions, emphasizing how environmental and operational parameters influence corrosion rates and scale formation. The analysis draws on laboratory studies that identify key controlling factors, with particular focus on precipitation at the metal wall, film protectiveness, and scale degradation under different flow regimes. The literature is critically evaluated with respect to temperature, CO2 partial pressure (PCO2), salinity, pH, and hydrodynamic effects. The reviewed studies confirm that these parameters strongly govern CO2 corrosion rates and scale development. Protective FeCO3 films typically form under favorable supersaturation and precipitation conditions, commonly at 60–90 °C, but are prone to destabilization under high shear stress or in acidic environments. At low salinity, chloride ions enhance corrosion, whereas at high salinity, reduced CO2 solubility lowers corrosion rates and promotes weakly adherent scale formation. At low concentrations, H2S can substantially suppress CO2 corrosion by promoting FeS film formation that restricts anodic dissolution. However, its influence on corrosion behavior is not uniform and varies with material grade, solution pH, and prevailing environmental conditions. Overall, this review advances understanding of CO2 corrosion mechanisms and processes in industrial systems, and delineates environmental thresholds governing protective scale stability in CO2-containing environments.